    red d arc gx300

    Hi I just picked up a used gx300 (ranger 305g) thats not working correctly. The machine runs great and the ac power works properly but the weld output will hardly spark till I turn past 7/8 of the output dial. Once i get power out of it theres no shortage of output but it still doesn't seem right, has a pretty rough arc. Anybody run into this issue? I cleaned the slip rings, brushes look good, had a look at the pc board and didn't see any obvious damage.

    Machine code is 11274 its a 2006 model has about 1700 hours on it.

  2. #2

    Re: red d arc gx300

    nobody has run into this before?

  3. #3
    Join Date
    Dec 2013
    Location
    Visalia, CA
    Posts
    1,633

    Re: red d arc gx300

    i wish i could help. but unfortunately i can only give this one a bump. keep reading, keep posting, keep trying.

    you have a well known machine and im sure help is soon to come
    bosses stuff:
    trailblazer 325
    maxstar 200

    my stuff:
    sa 200
    fronius transpocket 180
    100 amp Lincoln w/f
    97 f350 DIT

    Kevin

  4. #4

    Re: red d arc gx300

    So i haven't really had any time to work on this machine but I tried running an inverter and suitcase off the generator side of the machine and it wouldn't run worth a ****. plugged the same setup into the trailblazer and it ran fine. so obviously the ac output has issues too, would a bad board cause these issues or is it likely a problem with the generator itself?

  5. #5
    Join Date
    Dec 2013
    Location
    Texas
    Posts
    311

    Re: red d arc gx300

    Did you look at the board? Is there any signs of damage? Did you check any connections?
    68' redface
    64' redface
    78' blackface
    Squarewave 200
    Trailblazer 302
    Miller 12vs
    Millermatic 211
    Maxstar 150
    325 Xtreme
    Victor cut master 52
    Betenbender shear& brake
    Scotchman iron worker
    Wellsaw

  6. #6

    Re: red d arc gx300

    Quote Originally Posted by Brettliv View Post
    Did you look at the board? Is there any signs of damage? Did you check any connections?
    Didn't see any noticeable damage to the board. Pulled the connections and cleaned them but they looked ok

  7. #7

    Re: red d arc gx300

    Bump. I still haven't had any time to fix this yet, anyone have any ideas?

  8. #8

    Re: red d arc gx300

    bump.

  9. #9
    Join Date
    Apr 2015
    Location
    MS
    Posts
    1,560

    Re: red d arc gx300

    Have you checked your AC output with a DVOM to see what it is doing?


    Sent from my iPhone using Tapatalk
    The only constant in life is there is never enough chains

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement