Stick welding question.
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 12 of 12
  1. #1
    Join Date
    Mar 2010
    Location
    A-town KY
    Posts
    229

    Stick welding question.

    Hello all i have a question. My grandfather has a craftsman 230 amp AC arc (stick) welder. Can i weld a 1/4 inch aluminum oil pan with that? what rods would be best?
    Current welder
    Hobart Handler 187

    Dead welders
    HF 151 dual mig
    Craftsman Welder 20511
    Craftsman Welder 80amp Flux

    I killed them LOL!!!!

  2. #2
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    219

    Re: Stick welding question.

    sure you can, cant remember the last time i seen an aluminum rod. but they are out there.

    Also, just cause it can be done doesn't mean it should. i wouldn't even attempt such a thing
    syncro 250
    tb325
    bobcat 225plus
    miller 252
    ln25
    ellis 1600
    pm65
    ppllc/candcnc table
    jd2
    ta95s
    south bend lathe
    cheap mill

  3. #3
    Join Date
    Jun 2015
    Location
    Alaska born, Alaska bred
    Posts
    786

    Re: Stick welding question.

    Aluminum stick rod sucks. It's absolutely horrible. It is a last ditch effort, "we need to get this thing repaired ASAP or this boat is going down" type of welding. It is absolutely worthless. You'll blow through 1/4" plate in a couple of inches.

    That said, I've never heard of AC aluminum rod. I've only seen DC.
    2000 Lincoln SA-250
    1974 Miller Dial-Arc 250

  4. #4
    Join Date
    May 2010
    Location
    laguna niguel, Ca USA
    Posts
    1,181

    Re: Stick welding question.

    Ship pan to me I will weld it up

    Sent from my LG-K550 using Tapatalk
    Miller Xmt 350
    Lincoln Ln-25
    Ahp 200x
    Smith Gas Mixer AR/H
    Tig is my Kung Fu
    Throwing down dimes and weaving about
    Instagram http://instagram.com/weldor_wes
    WeldorWes@WcWeldingLLC.com

  5. #5
    Join Date
    Jun 2015
    Location
    Alaska born, Alaska bred
    Posts
    786

    Re: Stick welding question.

    Ship an oil pan from Kentucky to California for a weld?

    Surely there is at least one decent welder in his own state?
    2000 Lincoln SA-250
    1974 Miller Dial-Arc 250

  6. #6
    Join Date
    May 2010
    Location
    laguna niguel, Ca USA
    Posts
    1,181

    Re: Stick welding question.

    Quote Originally Posted by Hillbilly Welder View Post
    Ship an oil pan from Kentucky to California for a weld?

    Surely there is at least one decent welder in his own state?
    Not saying there isn't one was just an offer

    Sent from my LG-K550 using Tapatalk
    Miller Xmt 350
    Lincoln Ln-25
    Ahp 200x
    Smith Gas Mixer AR/H
    Tig is my Kung Fu
    Throwing down dimes and weaving about
    Instagram http://instagram.com/weldor_wes
    WeldorWes@WcWeldingLLC.com

  7. #7
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,535

    Re: Stick welding question.

    Quote Originally Posted by Hillbilly Welder View Post
    Aluminum stick rod sucks. It's absolutely horrible.
    Yes it is!
    Attached Images Attached Images    
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  8. #8
    Join Date
    Jun 2010
    Location
    northern cal.
    Posts
    208

    Re: Stick welding question.

    Do you have any idea how to "weld"? Not as easy as it appears.

  9. #9
    Join Date
    Oct 2016
    Location
    countryside of NY
    Posts
    143

    Re: Stick welding question.

    That is frist I ever seen stick weld aluminum. I had seen done with MIG or tig using AC .
    Nice weld cep
    MM215

  10. #10
    Join Date
    Jun 2012
    Location
    Ct
    Posts
    1,518

    Re: Stick welding question.

    I've done it a few times myself, its surprising how fast the rod burns up, you have to fall on top of it to keep the arc tight enough. It is messy, and the slag isn't easy to see through.



    Sent from my SAMSUNG-SM-G890A using Tapatalk

  11. #11
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,454

    Re: Stick welding question.

    Quote Originally Posted by mafiacustomz View Post
    Hello all i have a question. My grandfather has a craftsman 230 amp AC arc (stick) welder. Can i weld a 1/4 inch aluminum oil pan with that? what rods would be best?
    Because you have an AC welder, the answer would be no. The rods are all DC rods from what I've seen.

    I've done this a few times - thinnest being 1/8" material.

    As said above, it's not fun.

    It would be fine with a spool gun on a mig, but I much prefer TIG.
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  12. #12
    Join Date
    Oct 2016
    Location
    countryside of NY
    Posts
    143

    Re: Stick welding question.

    Oh hi dave. That's is a very sound advice.
    MM215

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement