    Hi All,

    Quick question. I am welding up a 6' lawn roller and just have a Lincoln Mig Pak 140 at my disposal. Can I do i with mig and thicker wire or should I just go all out with flux. Everything is 1/4" mild steel. Since it is an implement it needs to be strong. I am also welding end caps on the main roller and it needs to be watertight. When I run mig I use 75/25 if that helps at all.

    Thanks,
    gator

  2. #2
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    7,364

    Re: Lincoln Mig Pak 140 Welding 1/4"...Flux or Mig?

    It should have the parameters on the door chart- if they still have the chart on the door. Might be in the manual.


    wäter tight is all up to your skills-doesn't matter Mig or Fluxore
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Miller 125c Plasma 120v
    SO 2020 bender
    Beer in the fridge

  3. #3

    Re: Lincoln Mig Pak 140 Welding 1/4"...Flux or Mig?

    Yeah I forgot about that...Looks like it'll be flux Some guys really like flux but I prefer mig! Alot cleaner. Thanks maybe I'll post some pics when I finish it.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement