    Smaw 3g plate test

    Finally got around to doing my SMAW 3G limited thickness plate test. Here are some pics. Constructive criticism welcome.

    ROOT:
    Name:  1523088777665.jpg
Views: 183
Size:  35.3 KB

    FILL:
    Name:  1523088777536.jpg
Views: 168
Size:  35.3 KB
    Trailblazer 325 EFI
    Multimatic 200
    S32P-12
    Syncrowave 210 w/ MIG package
    Spoolmate 100
    Hypertherm Powermax 30 Air
    Burnt gloves & hands

  2. #2
    Join Date
    Jan 2017
    Location
    Hawaii
    Posts
    143

    Re: Smaw 3g plate test

    CAP:
    Name:  1523088775234.jpg
Views: 157
Size:  36.5 KB

    BENDS:
    Name:  1523237263570.jpg
Views: 155
Size:  12.0 KB

    Name:  1523236947231.jpg
Views: 156
Size:  11.2 KB

    I feel like my root went in fairly well. But my fill and cap needs improvement. Very slight undercut on the toes, should have held them longer.
    Trailblazer 325 EFI
    Multimatic 200
    S32P-12
    Syncrowave 210 w/ MIG package
    Spoolmate 100
    Hypertherm Powermax 30 Air
    Burnt gloves & hands

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement