    This is a warehouse that stores and maintains an insane amount of equipment for FDNY special operations and and FEMA Task Force 1.

    They have around 30 of these 30 horse outboard motors and rolling racks. The racks have very little support and can tip over easily when pulling the cord to start the motors for maintenance.

    There is around 10 racks so rather than modify each one, I devised these little quick connecting outriggers for use on whichever rack is currently being tested.

    Was able to make it 100% from scrap luckily because acquiring materials is a big production.

    Admittedly after being so satisfied how they turned out I realized I had made a grave mistake and had to add 2” to each one. I mistaked 12.5” in my drawing for what should have been 1’ 2.5”

    In retrospect I really should have beveled the plate with the long weld on both sides or put a fillet inside. I got lazy. It may snap off over time from the force of the bolts clamping it but we shall see.

    Never the less, just bee d to make some T bolts to clamp then on and off by hand and they should be all set.

    Name:  C37BB101-B5A7-483A-A554-11BB972B84FF.jpg
Views: 411
Size:  111.7 KB
    Name:  E097ABDF-A1E2-41B8-AC57-22481DCB9BDB.jpg
Views: 402
Size:  149.2 KB
    Name:  E0FD6191-099A-41F1-BDAE-2F3083973B6B.jpg
Views: 400
Size:  90.1 KB
    Name:  55AA3052-DCA0-4103-A2D4-82AF0813C435.jpg
Views: 404
Size:  156.3 KB
    Name:  E3C863B4-C173-4125-9C83-057E7D38DD33.jpg
Views: 403
Size:  152.2 KB
    Last edited by BrooklynBravest; 04-11-2018 at 05:25 PM.

  2. #2
    Join Date
    Oct 2013
    Location
    Long Island, NY
    Posts
    1,813

    Re: Outboard Motor Rack Support

    Name:  2187D11E-62A5-4CA2-9B85-22D7DB88C796.jpg
Views: 388
Size:  93.6 KB
    Name:  A14EFD5A-63BC-406A-9CDE-E44BAB96B81E.jpg
Views: 392
Size:  142.1 KB
    Name:  7D21C92F-A96A-4681-B1FB-41EA105E289D.jpg
Views: 393
Size:  200.1 KB
    Last edited by BrooklynBravest; 04-11-2018 at 05:20 PM.
    www.FirehouseFabricators.com



    Lincoln 210mp
    Lincoln SW200

  3. #3
    Join Date
    Jan 2012
    Location
    West Rutland, Vermont
    Posts
    113

    Re: Outboard Motor Rack Support

    Excellent simplistic problem solving.

  4. #4
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,452

    Re: Outboard Motor Rack Support

    Wait a minute. It appears to me that you are showing off those fancy Magswitches.

    I had a similar setup I did. I used square tube And cut open one side instead of welding angle and flat stock. I drilled hole in one side, welded Extraheavy nut over hole. Then used Bolt to lock down. Holding up well.

  5. #5
    Join Date
    Oct 2013
    Location
    Long Island, NY
    Posts
    1,813

    Re: Outboard Motor Rack Support

    Quote Originally Posted by BD1 View Post
    Wait a minute. It appears to me that you are showing off those fancy Magswitches.

    I had a similar setup I did. I used square tube And cut open one side instead of welding angle and flat stock. I drilled hole in one side, welded Extraheavy nut over hole. Then used Bolt to lock down. Holding up well.
    That was my original plan but I did not have suitable tube scrap in that size.

    The magswitches have been great I may order big ones.
    www.FirehouseFabricators.com



    Lincoln 210mp
    Lincoln SW200

  6. #6
    Join Date
    Sep 2005
    Location
    Cave Creek AZ
    Posts
    2,612

    Re: Outboard Motor Rack Support

    That is a very elegant solution, nice work!

  7. #7
    Join Date
    Oct 2013
    Location
    Long Island, NY
    Posts
    1,813

    Re: Outboard Motor Rack Support

    All done.

    Doesn’t budge at all especially if the rack has motors on it. Just needed that little bit of extra support.

    Name:  B3365D06-62D2-4C1C-AD76-4D47BC68E89A.jpg
Views: 185
Size:  165.1 KB
    Name:  6FA29D5D-2395-4006-8941-61FF6C2442BF.jpg
Views: 183
Size:  121.6 KB
    www.FirehouseFabricators.com



    Lincoln 210mp
    Lincoln SW200

  8. #8
    Join Date
    Dec 2008
    Location
    Long Island, NY
    Posts
    571

    Re: Outboard Motor Rack Support

    Nice work. Looks good - bet they appreciate having them.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement