    I picked up this VICTOR ETS4-125-590 regulator, but it seems the LP outlet has been modified from the original. I am trying to figure out what type of fitting I need for this outlet. The modified piece has a 317 with a word above it I can't make out. Any ideas?

    Name:  20180411_224806.jpg
Views: 195
Size:  49.9 KB

  2. #2
    Join Date
    Apr 2018
    Location
    TN
    Posts
    162

    Re: Cylinder Regulator Question

    You can pick up any fitting you need from your local welding supply. They used a gas fitting common to the cable you see here in my picture. Fyi, i had to change to that fitting to use it. Don't have a pic of the connector alone, but there is a double female coupling that connects the male to male ends you can see at the regulator on the hose.

    Name:  SmartSelectImage_2018-04-12-01-33-40.jpg
Views: 147
Size:  209.7 KBName:  SmartSelectImage_2018-04-12-01-30-31.jpg
Views: 148
Size:  202.2 KBName:  SmartSelectImage_2018-04-12-01-31-44.jpg
Views: 146
Size:  101.4 KBName:  SmartSelectImage_2018-04-12-01-31-30.jpg
Views: 146
Size:  537.5 KB
    Last edited by One1; 04-12-2018 at 01:39 AM.
    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  3. #3
    Join Date
    Oct 2014
    Posts
    127

    Re: Cylinder Regulator Question

    Or get the correct piece to go right in the regulator.


  4. #4
    Join Date
    Apr 2018
    Location
    TN
    Posts
    162

    Re: Cylinder Regulator Question

    Also acceptable but here's why that doesn't usually work. Most importantly the small harris regulators don't accept replacement fittings, so thats out entirely. You'll likely end up with one if you buy a porta-torch, any mig from most stores, and so forth. Most people end up having multiple Regulators multiple tanks multiple hoses and all of them have male fittings but most of the Regulators also have male fittings like the hoses so if you go ahead and buy yourself a coupler you can swap tanks and hoses and Regulators easily without having to go out and buy a new fitting every single time you buy a regulator. As below, the same hose on my larger tank and flowmeter. Tanks 2 of 5. Swapping easily using the coupler.

    I don't know your situation in your original post. If you're just getting a regulator, you'll likely get more. I'd try to be as diverse as possible, myself.

    Name:  20180412_170921.jpg
Views: 101
Size:  73.7 KB
    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

  5. #5
    Join Date
    May 2014
    Location
    Central Wa. state
    Posts
    1,578

    Re: Cylinder Regulator Question

    37 degree JIC fitting, mostly used for hydraulics. Check the range of the Low pressure gauge, it may be a Nitrogen regulator for charging hydraulic accumulators. Ithink mine has a low pressure gauge that goes to 2500 PSI.

  6. #6

    Re: Cylinder Regulator Question

    Quote Originally Posted by 12V71 View Post
    37 degree JIC fitting, mostly used for hydraulics. Check the range of the Low pressure gauge, it may be a Nitrogen regulator for charging hydraulic accumulators. Ithink mine has a low pressure gauge that goes to 2500 PSI.
    The 37 degree JIC fitting looks right. It was originally an industrial air regulator with a working pressure is 5 - 125 psig and the LP gauge reads up to 200 psi. I will be taking it into to the local welding supply store to see about getting the right adapter. Thanks

  7. #7

    Re: Cylinder Regulator Question

    Thank you all for the info. I have everything hooked up without any leaks now. Cheers

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement