    Getting materials together to build a BBQ smoker; trying to keep cost and weight down. I've used 3/8" round bar carbon steel to make a darn nice cooking grate to use over a campfire. It works and looks awesome, isn't super heavy, and cost next to nothing. Question is: would 3/8" be thick enough for a charcoal basket for my smoker, or should I jump up to 1/2" or even 5/8"?

  2. #2
    Join Date
    Oct 2013
    Location
    Long Island, NY
    Posts
    1,813

    Re: Cooking grate/Charcoal basket

    It’s probably more than thick enough...

    You’re building a basket for hot coals, not a forge.

    1/8” rod would probably suffice from the standpoint of surviving the coals.
    www.FirehouseFabricators.com



    Lincoln 210mp
    Lincoln SW200

  3. #3
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    2,880

    Cooking grate/Charcoal basket

    Hate to disagree,
    But I think 3/8 will twist like a pretzel after a few hours of red hot coals.

    I used 5/16 round for my firebox grate and it warped to all hell... (leftover material from my sliding cooking /food grate)

    I think 3/8 will do the same.

    I'm gonna make another one this summer using 1/2 or larger.... whatever I can get at the steel depot.

    I use basically wood, but I don't think the heat difference is much charcoal briq. vs wood

    Last edited by John T; 04-13-2018 at 02:52 PM.
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.


  4. #4
    Join Date
    Nov 2005
    Location
    ca
    Posts
    11

    Re: Cooking grate/Charcoal basket

    I used heavy epanded metal. Worked fine for years.
    Syncrowave 250 w/ coolrunner
    MM210
    SP 135
    Victor O/A

  5. #5
    Join Date
    Nov 2014
    Location
    PDX PNW
    Posts
    5,516

    Re: Cooking grate/Charcoal basket

    I just put my wood straight on firebrick. U could do the same With briquettesName:  IMG_7916.jpg
Views: 359
Size:  96.9 KBName:  IMG_7551.jpg
Views: 360
Size:  153.7 KBwelcome to the forum
    Last edited by motolife313; 04-14-2018 at 12:40 AM.

  6. #6

    Re: Cooking grate/Charcoal basket

    Quote Originally Posted by John T View Post
    Hate to disagree,
    But I think 3/8 will twist like a pretzel after a few hours of red hot coals.

    I used 5/16 round for my firebox grate and it warped to all hell... (leftover material from my sliding cooking /food grate)

    I think 3/8 will do the same.

    I'm gonna make another one this summer using 1/2 or larger.... whatever I can get at the steel depot.

    I use basically wood, but I don't think the heat difference is much charcoal briq. vs wood

    I looked back at the camping grate I made and turns out it’s 1/4”. It’s done well being in the flames, but has always been pretty far from the hot embers. I’ve seen a rebar poker turn red hot stuck down in there. Steel supplier has solid round up to an inch pretty darn cheap. Maybe I’ll go for 1/2”?

    By the way, that’s an awesome rig you built. I’m just tryin to have some delicious meat, yours looks like you could feed a company of infantrymen!
    Last edited by laxphatty; 04-14-2018 at 03:20 AM.

  7. #7

    Re: Cooking grate/Charcoal basket

    Quote Originally Posted by Tbones View Post
    I used heavy epanded metal. Worked fine for years.
    My supplier has sheets of flat expanded. 4’x6’ (I think) with 3/4” gap for $54. It wasn’t labeled, but my thickness gauge put it at about to be 11g. It looked beefy enough, but not sure given the opinions against 3/8” solid rod here...

  8. #8

    Re: Cooking grate/Charcoal basket

    Quote Originally Posted by motolife313 View Post
    I just put my wood straight on firebrick. U could do the same With briquettesName:  IMG_7916.jpg
Views: 359
Size:  96.9 KBName:  IMG_7551.jpg
Views: 360
Size:  153.7 KBwelcome to the forum
    I’m making an Ugly Drum Smoker. Nowhere near as sophisticated as yous

  9. #9
    Join Date
    Aug 2012
    Posts
    15

    Re: Cooking grate/Charcoal basket

    The expanded stands a better shot. I've made a few of fire baskets with different sizes expanded grate. The thicker the better of course, can frame it in with tube or weld it to itself. The expanded doesn't warp or sag as much as rod cause of the amount of support in many directions.

    Sent from my SAMSUNG-SM-G930A using Tapatalk

  10. #10
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    2,880

    Re: Cooking grate/Charcoal basket

    Had they day off today so I drug the smoker out of the woods...
    Got 3 racks of ribs on for about 3 hours now @ 250 ish

    Gettin ready to wrap em up for prolly and hour and half...


    Heres my grate..
    Probably wouldn’t have warped if I ran support down the middle

    But it gets the job done..







    Sent from my iPhone using Tapatalk Pro
    Miller 211
    Hypertherm PM 45
    1961 Lincoln Idealarc 250
    HTP 221


    True Wisdom only comes from Pain.


Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement