Wilson Plastic-Arc
RSS | Subscribe | Contact Us | Advertise | About Us
Results 1 to 8 of 8
  1. #1
    Join Date
    Aug 2010
    Location
    St. Paul MN
    Posts
    13

    Wilson Plastic-Arc

    Rescued this one. Built sometime in the 20’s from what I can tell.


  2. #2
    Join Date
    May 2015
    Location
    Eastern Oregon
    Posts
    249

    Re: Wilson Plastic-Arc

    That is neat. Thanks for sharing.

  3. #3
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,318

    Re: Wilson Plastic-Arc

    DC? How many amps is she rated at?
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Victor O/A setup
    Makita chop saw

  4. #4
    Join Date
    Aug 2008
    Posts
    11,007

    Re: Wilson Plastic-Arc

    "Any day above ground is a good day"

    http://www.farmersamm.com/

  5. #5
    Join Date
    May 2016
    Location
    NW OH
    Posts
    233

    Re: Wilson Plastic-Arc

    That thing is awesome. Got any details or story behind your acquisition/rescue?

  6. #6
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    160

    Re: Wilson Plastic-Arc

    Early 1900s machine, made in NY City.
    Wilson appears to have been going head to head with Lincoln on the US side of the ocean to get into the welded steel ocean ship hull business that was then just beginning.

    Some Wilson information is in the Smithsonian collection.

    Somebody found this book and generously put it on line.
    https://ia801404.us.archive.org/1/it...00wilsrich.pdf

    The Library that has it says the file may have been damaged. It sure don't like to load easily.

  7. #7
    Join Date
    Aug 2006
    Location
    St. Paul Park MN
    Posts
    817

    Re: Wilson Plastic-Arc

    Quote Originally Posted by mla2ofus View Post
    DC? How many amps is she rated at?
    Mike
    Its a 300 amp machine.

  8. #8
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,245

    Re: Wilson Plastic-Arc

    That's pretty cool
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement