    D ring support

    Hi there - I have a dump trailer that needs D rings welded. I want to weld them on to the sides in the rear so they don't interfere with a load of aggregate but have enough strength to hold a compact tractor.
    The sides are 2x4 1/8" post with 12 gauge sheeting.

    Question is should I simply weld on a 1/2" D ring right to the 12 gauge sheet at the inside of the post?
    Or should there be some other backer plate? Or should I possibly drill a hole and weld in a tube through the 2x4 to tie it all in?

    Just worried that it may try to rip the 12 gauge sheet away from the post.

    Thanks

  2. #2
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,724

    Re: D ring support

    I would weld the D-rings to a plate, then use another plate, so you can sandwich the 12-GA sheet metal. Use 4-bolts to tie the two plates together.
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  3. #3
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,452

    Re: D ring support

    As stated above. Bolt on " D" rings and backup behind.

  4. #4
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,964

    Re: D ring support

    Quote Originally Posted by CEP View Post
    I would weld the D-rings to a plate, then use another plate, so you can sandwich the 12-GA sheet metal. Use 4-bolts to tie the two plates together.
    That kicked loose a random memory rattling around my head from the 80's.....

    When sandwiching plates on thin metal, the plates should be different sizes to help eliminate the shearing effect (like a scissors).

    This was from theory of installing bolted plates for roll bars on mud trucks back then.

    It could have been wrong, or could have changed by now

    Anyone know of similar from a modern reference?
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  5. #5

    Re: D ring support

    I wanted to put it right at a post so it would be difficult to get a plate behind unless I fish it down the post somehow.

  6. #6
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,724

    Re: D ring support

    I added D-rings to my dump trailer. It came with 4 D-rings on the corners. I used bolt on D-rings in the stake pockets.
    Attached Images Attached Images   
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  7. #7
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,964

    Re: D ring support

    Quote Originally Posted by CEP View Post
    I added D-rings to my dump trailer. It came with 4 D-rings on the corners. I used bolt on D-rings in the stake pockets.
    Bolted on.... I wonder if moderators can take away your hobby status...
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  8. #8
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,431

    Re: D ring support

    Bust down to Solderer I'd say.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  9. #9

    Re: D ring support

    Quote Originally Posted by MinnesotaDave View Post
    Bolted on.... I wonder if moderators can take away your hobby status...
    okay bolted on it is. thanks for the ideas.

  10. #10
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,964

    Re: D ring support

    Quote Originally Posted by farmerwellder23 View Post
    okay bolted on it is. thanks for the ideas.
    Hey now, bolting stuff on is a termination type offense on a welding website

    We'll have to bust CEP back down to a no-stripe recruit in basic training for even suggesting it
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  11. #11
    Join Date
    Jun 2014
    Location
    Southern Illinois
    Posts
    368

    Re: D ring support

    I can’t imagine CEP wanting to run any of his pristine engine drives for a mere D ring job. Lol


    Sent from my iPhone using Tapatalk
    Steve

    Miller Dialarc 250 (1990)
    Miller Maxstar 140 STR (2003)
    Lincoln SA200 Redface Pipeliner (1966)
    Lincoln MP210 (2015)
    Victor and MECO torches

  12. #12
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,964

    Re: D ring support

    Quote Originally Posted by Sparkie1957 View Post
    I can’t imagine CEP wanting to run any of his pristine engine drives for a mere D ring job. Lol


    Sent from my iPhone using Tapatalk
    Ya, they might get dirty Ha!
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  13. #13
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,431

    Re: D ring support

    But think of all the new bead sample photos he couldv'e posted up.

    Probably above his skill level anyhow.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

  14. #14
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    12,964

    Re: D ring support

    Quote Originally Posted by duaneb55 View Post
    But think of all the new bead sample photos he couldv'e posted up.

    Probably above his skill level anyhow.
    Pfftttt--bahhahahahah!
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  15. #15
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    9,724

    Re: D ring support

    What’s going on here? Is this pick on CEP day?
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  16. #16
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,431

    Re: D ring support

    I didn't say nothin' . . .
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save Second Base!

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement