    I came a little to close for comfort to a overheating condition today. I'm looking for ideas to help stay cool or cooler. I'm thinking maybe linen shirt under my jacket but looking for other ideas. I've heard of the miller cool belt but not sure if I can use it with a speedglas helmet.

    Thanks in advance for ideas

    Sent from my SM-N950U using Tapatalk

  2. #2
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: Staying cool under the hood

    If you're close to a clean air supply you can use one of these:

    https://www.vortec.com/cooling-only-pac/overview

    I made a hose assembly to connect to it that I put on like a harness under my shirt. Put some holes in it for the cool air to blow next to my torso, the thing is a lifesaver for an old fart like me in the Texas summer heat.

  3. #3
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    77

    Re: Staying cool under the hood

    Look up cooling vests on ebay.
    They come in both air cooled and water cooled.
    You get lucky somebody is selling the government surplus vests from Operation Desert Storm.

  4. #4
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: Staying cool under the hood

    Don't get one of those ice pack vests, they don't stay cold very long and the get real swampy.

  5. #5
    Join Date
    Dec 2014
    Location
    Northern California
    Posts
    84

    Re: Staying cool under the hood

    Name:  62FC10AE-5D41-456B-BEF2-9CAACC217748.jpg
Views: 141
Size:  78.1 KB

    Get a forced air hood...it will save your lungs too. I got headaches and sweaty...this fixed both problems.

  6. #6
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: Staying cool under the hood

    That thing might work in Northern California, but it don't do squat in South Texas for heat. I know, I use one.

  7. #7

    Re: Staying cool under the hood

    Quote Originally Posted by Tarmstrong View Post
    Name:  62FC10AE-5D41-456B-BEF2-9CAACC217748.jpg
Views: 141
Size:  78.1 KB

    Get a forced air hood...it will save your lungs too. I got headaches and sweaty...this fixed both problems.
    What kind is that? Looks like it will fit on my speedglas

    Sent from my SM-N950U using Tapatalk

  8. #8
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    1,804

    Re: Staying cool under the hood

    Back in the FL daze during Oven( July-Aug-Sept), I'd go in at 3-4 in the morning and strike an arc.I'd have all kinds of crap tacked up the afternoon before and up on saw horses. 3-4 hours of MIG on WFO is a lot of feet of weld. Then toss paint, fill columns with concrete and go back under the shed roof and play with the Scotchman and K-zoo and get a bunch of other crap tacked up and ready to go. The shop there was just like this one except 6 times larger and 8 feet taller.
    Here I wear a beanie thingie the guys from Blue Demon sell it has some kind of goop that reacts with water and chills it. Like Gadaffi meets Carharrt.
    Name:  91RszofPjIL._SL1500_.jpg
Views: 136
Size:  70.2 KB

  9. #9
    Join Date
    Mar 2018
    Location
    Tampa, Florida
    Posts
    170

    Re: Staying cool under the hood

    Quote Originally Posted by Bonzoo View Post
    Here I wear a beanie thingie the guys from Blue Demon sell it has some kind of goop that reacts with water and chills it. Like Gadaffi meets Carharrt.
    Name:  91RszofPjIL._SL1500_.jpg
Views: 136
Size:  70.2 KB
    So this thing-a-majig works good, is comfortable, and is pretty durable Mr.Bonzoo? Hot slag and berries won’t burn through and cause it’s innards to run down my face? If so I may consider getting one. Especially when Im Sitting down to some TIG in the garage and cant have any air movement at the welding table. The “oven” is set on pre-heat already!
    -Mark Smith

    Vulcan ProTig200
    Everlast Powertig 185DV

  10. #10
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    1,804

    Re: Staying cool under the hood

    Quote Originally Posted by Mmock4 View Post
    So this thing-a-majig works good, is comfortable, and is pretty durable Mr.Bonzoo? Hot slag and berries won’t burn through and cause it’s innards to run down my face? If so I may consider getting one. Especially when Im Sitting down to some TIG in the garage and cant have any air movement at the welding table. The “oven” is set on pre-heat already!
    I have Coconut Head for doing Over Head so I never showered it with sparks but it washes up( by hand) real well and is super comfortable under the band. Sitting at the table, it's killer.I may even wear it to church !

  11. #11
    Join Date
    Nov 2012
    Location
    South Texas
    Posts
    2,127

    Re: Staying cool under the hood

    Quote Originally Posted by formernuke View Post
    What kind is that? Looks like it will fit on my speedglas

    Sent from my SM-N950U using Tapatalk
    That thing just blows the outside air through a filter into your hood. It doesn't have any kind of cooling with it. If the air around you is hot, that's what you get. I've been using one for about 3 years, it's great for keeping smoke out of your lungs, but it doesn't cool you off when it's hot and humid.

  12. #12

    Re: Staying cool under the hood

    Mate I have had enough days welding in the Australian summer heat to know exactly how you feel. I got a new Speedglas hood with Adflo at the end of last year, coming into the hot season... it seriously changed everything. 100% worth looking at and it also keeps the black crap out of the nose. This is the one I got https://www.awsi.com.au/welding-helm...9100xxi-507726

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement