Rusty stainless steel handrail - Page 2
RSS | Subscribe | Contact Us | Advertise | About Us
Page 2 of 2 FirstFirst 12
Results 26 to 28 of 28
  1. #26
    Join Date
    May 2017
    Posts
    11

    Re: Rusty stainless steel handrail

    Ya I used I regular steel wire wheel without realizing it. I got most of the rust out with acetone and scotch brite pad then a stainless steel wire wheel. It's 90% gone so I'll repeat the process and see how much I can get out.

  2. #27
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    6,952

    Re: Rusty stainless steel handrail

    Spend $2. on some Barkeeper's Friend.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  3. #28
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    2,868

    Re: Rusty stainless steel handrail

    Quote Originally Posted by Oldendum View Post
    Spend $2. on some Barkeeper's Friend.
    That's what I would do. Get the POWDER formula, not the liquid. And mix it so that it's more of a paste. Even better, mix it with lemon juice instead of water, and apply it hot.

    It won't truly passivate, the the oxalic acid does a good job of removing the oxide, and if done well enough, the steel should passivate itself in the open air. That is unless you're in a marine environment where 316 would have been more appropriate than 304 which doesn't deal as well with the salt air.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement