    Passivation products

    Does anyone know where I can buy some stainless steel passivaton products in Vancouver or maybe online? Or can I DIY it? I tried to clean rust off a stainless handrail I made but it just came back, used citric acid dissolved in tap water with an electrified wand.

  2. #2
    Join Date
    Oct 2015
    Location
    PNW
    Posts
    342

    Re: Passivation products

    i tried a homemade electric wand/ citric thing and failed. parts pads etc are crazy expensive and slow to use.

    now if pieces are small enough i heat in a citric bath, if bigger use pickling paste and a fleece (scotchbrite) pad on a burnisher.

    definitely a learning process but recently got this 10,000 gal tank passed inspection for a local water dept.


    Name:  IMG_20180607_145952721_HDR.jpg
Views: 163
Size:  200.5 KB
    General Contractor
    Commercial Industrial & Custom Residential
    Specializing in all things Metal

  3. #3
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    6,951

    Re: Passivation products

    I've heard of using hot citric acid, but not with an electrolytic wand. I have heard of using phosphoric acid solution with a wand, but generally to get rid of welding heat tint.

    Have you tried oxalic acid? (not with a wand)
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  4. #4
    Join Date
    Nov 2016
    Location
    Mars
    Posts
    18

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement