    Dual Argon regulator connection

    I have a question on connecting 2 regulators to a single Argon tank. I have a typical single out flow meter (with ball) and an argon flow gauge (gauge type). Is it safe to run a normal tank adapter to an ips tee then a short nipple to both regulators? I know this is a simple question, but I've never seen it done this way and I'm going to go plumping on the high side of the regulator without knowing for sure it's alright.

    Thanks to anyone who takes the time to help. Appreciate it.

  2. #2
    Join Date
    Mar 2017
    Location
    bar stool
    Posts
    162

    Re: Dual Argon regulator connection

    Unless you require different gas pressures from each regulator you'll be better off going cylinder > regulator > T > 2 flowmeters on the low pressure side.

  3. #3

    Re: Dual Argon regulator connection

    I agree and can't think of reason I would need to do so (which is probably the reason I haven't seen this done) but I was hoping to make use of the materials I have if safe to do so.

  4. #4
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    156

    Re: Dual Argon regulator connection

    You must want run 2 machines off of 1 tank? Yes you can do it. I have a Gas Mixer hooked to one side of a Tee on an argon tank and a flowmeter on the other for my Tig rig. Done it for years. Just make sure that the Tee is rated for the tank pressure. I don't think I would build a Tee out of plumbing pipe. Good Luck..
    Thermal Arc 320SP
    Cobra Pythons
    Thermal Arc 300 AC/DC
    Thermal Arc 161STL
    Thermal Arc 190S
    Cut Master 82, 42.
    Victor Gas App.
    Ellis 1600
    Evolution Compound Mitre.
    Boxes of welding crap.

  5. #5
    Join Date
    Apr 2010
    Posts
    55

    Re: Dual Argon regulator connection

    Just buy a double flow meter. I think there around $100 irc. Used all the time to run a purge and a torch.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement