    Chug chug chug goes the Pro mig 180

    Hi there:
    I am using Lincoln Electric Innershield flux core wire, .035 with my Pro mig 180
    and when laying a bead the wire is chugging. It's not bouncing like the wire speed is to high but will just chug. You can hear it and see the wire bouncing but not like the wire feed is to high. Any suggestions to correct this problem? I don't hear the bacon frying sound but I hear chug, chug chug. TIA.

  2. #2
    Join Date
    Dec 2007
    Location
    Los Angeles
    Posts
    7,173

    Re: Chug chug chug goes the Pro mig 180

    How's the drive roll tension?
    Ed Conley
    http://www.screamingbroccoli.com/
    MM252
    MM211 (Sold)
    Passport Plus & Spool gun
    Lincoln SP135 Plus- (Gone to a good home)
    Miller 125c Plasma 120v
    SO 2020 bender
    Beer in the fridge

  3. #3
    Join Date
    Jun 2018
    Location
    Knoxville TN
    Posts
    18

    Re: Chug chug chug goes the Pro mig 180

    Are you using the knurled drive roller?
    Try changing tips. Sometimes they bind up if the wire burns back too far.

  4. #4

    Re: Chug chug chug goes the Pro mig 180

    Check your wire liner sounds like it dirty
    All you need to do is clean your wire liner

    Dave

    Quote Originally Posted by Hollis View Post
    Hi there:
    I am using Lincoln Electric Innershield flux core wire, .035 with my Pro mig 180
    and when laying a bead the wire is chugging. It's not bouncing like the wire speed is to high but will just chug. You can hear it and see the wire bouncing but not like the wire feed is to high. Any suggestions to correct this problem? I don't hear the bacon frying sound but I hear chug, chug chug. TIA.

  5. #5
    Join Date
    Mar 2018
    Posts
    22

    Re: Chug chug chug goes the Pro mig 180

    Quote Originally Posted by Broccoli1 View Post
    How's the drive roll tension?
    It checks to be alright but I will check it again. Thanks

  6. #6
    Join Date
    Mar 2018
    Posts
    22

    Re: Chug chug chug goes the Pro mig 180

    Quote Originally Posted by smithdoor View Post
    Check your wire liner sounds like it dirty
    All you need to do is clean your wire liner

    Dave
    I will have a friend blow it out tomorrow when I see him. Thanks

  7. #7
    Join Date
    Mar 2018
    Posts
    22

    Re: Chug chug chug goes the Pro mig 180

    Quote Originally Posted by jfh View Post
    Are you using the knurled drive roller?
    Try changing tips. Sometimes they bind up if the wire burns back too far.
    I don't think the Knurled drive roller is being used. Not sure if
    I have one or not. I will check. Thanks.

  8. #8
    Join Date
    Mar 2018
    Posts
    22

    Re: Chug chug chug goes the Pro mig 180

    I saw a youtube video of a fella from Lincoln electric say that the stick out of that wire should be 1/2" to 5/8" but when I have it less than that (maybe 5/16" to 3/8") it wont chug. Wont that short of a stick out hurt anything?

  9. #9
    Join Date
    Aug 2008
    Posts
    11,095

    Re: Chug chug chug goes the Pro mig 180

    Innershield will run on rust. But it will be erratic, as you're seeing maybe.

    I occasionally have the pulsing problem you describe. Flap wheel to shiny metal usually helps. And, although contra-intuitive, and against all advice....reducing stickout below recommended length goes a long way in producing a more consistent weld, with less pulsing, when using Innershield 211, or other types of filler that are similar.

    What you do when you reduce stickout is increase the amps, and it can either help you, or hurt you. Just be careful not to ground your tip, that can get expensive if it blows something in the machine. Not all machines are created equal. I had a Hobart guy tell me that excessive grounding can mess up a rectifier bridge (?) whatever that is. I grounded a tip while tacking, and forgot I was using a wire welder, and alls I had to do was release the trigger instead of trying to yank it off the steel where it had stuck when grounded. And there weren't no squeezy thingy to let loose of the rod from the stinger either Anyways......I looked inside the machine, and the connector thingies were ok at the rectifiers.....whew!!!!!! Tech help at Hobart is very good, it keeps me coming back to them when I need a new machine.

  10. #10
    Join Date
    Mar 2018
    Posts
    22

    Re: Chug chug chug goes the Pro mig 180

    Quote Originally Posted by farmersamm View Post
    Innershield will run on rust. But it will be erratic, as you're seeing maybe.

    I occasionally have the pulsing problem you describe. Flap wheel to shiny metal usually helps. And, although contra-intuitive, and against all advice....reducing stickout below recommended length goes a long way in producing a more consistent weld, with less pulsing, when using Innershield 211, or other types of filler that are similar.

    What you do when you reduce stickout is increase the amps, and it can either help you, or hurt you. Just be careful not to ground your tip, that can get expensive if it blows something in the machine. Not all machines are created equal. I had a Hobart guy tell me that excessive grounding can mess up a rectifier bridge (?) whatever that is. I grounded a tip while tacking, and forgot I was using a wire welder, and alls I had to do was release the trigger instead of trying to yank it off the steel where it had stuck when grounded. And there weren't no squeezy thingy to let loose of the rod from the stinger either Anyways......I looked inside the machine, and the connector thingies were ok at the rectifiers.....whew!!!!!! Tech help at Hobart is very good, it keeps me coming back to them when I need a new machine.
    I have found that it does run erratic on rust and I from now on will use my flap disk to take off the rust and paint. I did ground the tip today and I was lucky not to ruin the machine. Thanks.

  11. #11

    Re: Chug chug chug goes the Pro mig 180

    Also look for a kink in liner too
    You can increase your tension or buy knurled drive roller but if in the liner it will make nest for you

    Typical use higher tension or knurled drive roller is for heavyer wire sizes

    Dave

    Quote Originally Posted by Hollis View Post
    I will have a friend blow it out tomorrow when I see him. Thanks

  12. #12
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    2,324

    Re: Chug chug chug goes the Pro mig 180

    Quote Originally Posted by Broccoli1 View Post
    How's the drive roll tension?
    Bingo ! Absolute minimal tension.Not near enough to curl the wire on a table adjust. Just a banana bend.

  13. #13
    Join Date
    Apr 2018
    Location
    TN
    Posts
    162

    Re: Chug chug chug goes the Pro mig 180

    I have bought 2 brand new Lincoln 180's (last one was last month so I'm still breaking it in). BOTH the one's I bought had bad tips. They were brand new, but wouldn't make decent contact with the wire for anything. I nearly sold my first one over it before I decided just cause it was new didn't mean it wouldn't fail. So...... put a new tip on and it welded like a dream. You may wanna do that and see just incase.
    1957 Lincoln Idealarc 300 AC/DC
    1971 Miller Thunderbolt 225
    2018 Lincoln 180
    2018 Lincoln 3350 papr

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement