    Wire Recomendations

    Opinions on the best

    Mig Wire and FluxCore Wire

    Are there any to avoid?
    Gregg

  2. #2
    Join Date
    Jun 2017
    Location
    AJO, ARIZONA
    Posts
    553

    Re: Wire Recomendations

    You'll pay more but you won't go wrong with Lincoln. I don't have any Lincoln mig wire, but have some Nr211 flux core, my mig wires are all Forney & Hobart & they are fine.
    NRA LIFE MEMBER
    UNITWELD 175 AMP 3 IN1 DC MIG/STICK/TIG
    MIDSTATES 300 AMP AC MACHINE
    GOD BLESS AMERICA!
    “Freedom is never more than one generation away from extinction.
    We didn’t pass it to our children in the bloodstream".
    RONALD REAGAN

  3. #3
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,746

    Re: Wire Recomendations

    I like the esab spoolarc 86 for mig hard wire. Much better pricing from my supplier and runs nicer than Lincoln l-56, which is also a decent wire.

  4. #4
    Join Date
    May 2010
    Location
    Sparks, NV
    Posts
    9,343

    Re: Wire Recomendations

    X2 on the Spoolarc 86
    Tiger Sales: AHP Distributor www.tigersalesco.com
    AHP200x; AHP 160ST; MM350P, Spoolmatic 30A; Everlast PowerTig 185; ESAB 875 plasma;Evo 355. OA

  5. #5
    Join Date
    Sep 2013
    Location
    west texas
    Posts
    2,302

    Re: Wire Recomendations

    Tried a few and the best for me has always been nr-211.
    old Miller spectrum 625
    Lincoln SP-135 T, CO2+0.025 wire
    Miller model 250 and WP-18V torch
    Craftsman 100amp AC/DC and WP-17V torch
    Century 115-004 HF arc stabilizer
    Home made 4 transformer spot welder
    Home made alternator welder

  6. #6
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,093

    Re: Wire Recomendations

    I like the Lincoln L 56 .

  7. #7

    Re: Wire Recomendations

    I TRY the low cost wire to save. Money

    When had shop I only one type of Type of wire E71T-1 with CO2 0.052 in 60 lb coils
    we use it for 1 1/2" plate to 16Ga

    Any other welding it was stick or torch

    Since I in California at any some X-ray the weld and would after it was done the weld pass.

    Dave

    Quote Originally Posted by Rangerhgm View Post
    Opinions on the best

    Mig Wire and FluxCore Wire

    Are there any to avoid?

  8. #8
    Join Date
    Mar 2012
    Location
    Australia
    Posts
    412

    Re: Wire Recomendations

    I'm a massive fan of anything made by ESAB, I've had alot of good experiences with they're spoolarc 86 for solid wire and they're duel shield wires are second to none, they're 7100 Ultra is the smoothest running duel shield wire I've ever used, with the exception of the Metrode supercore 316L (but stainless in general runs smooth), and they're 8000-B2 and 9000-B3 wire's despite being a high alloy wire for creep resistant steel (think boilers experiencing 2500+ PSI at 1100 degree's F) it welds very smooth and is easy to get very high deposition rates with good mechanical properties and very low chance of failures.

    most welder's don't realize that the term "duel shield" is actually a trademarked name by ESAB for they're gas shielded flux core wires, and the fact that "duel shield" has become the generic term for gas shielded flux core say's alot, similar to how most british people call every vacuum clean a "hoover", Lincoln call they're "duelshield" wires outershield for that reason. but everyone still calls it duel shield.

    Basically I highly recommend trying the ESAB wire, be it solid wire or any of they're other's, ESAB makes quality products.
    Last edited by ttoks; 08-12-2018 at 07:19 PM.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement