    Anyone know if the Power I-MIG 230 can do spray transfer?

    I keep reading it's a function of voltage output above 25 and the specs say it can deliver 25.5 but that's a slim margin.

    Opinions on this machine are welcome.

  2. #2
    Join Date
    Feb 2015
    Posts
    63

    Re: POWER I-MIG 230I & spray transfer

    Nope, very few welders under 250 amps can spray arc (it's not a function of the amps though, it is just only that machines above 250 amps generally also are designed to output higher voltage to spray). I believe the only Everlast welder that does spray arc comfortably is the 275. Maybe the 251Si can too, just can't remember off the top of my head.

    Otherwise for a sub 250 amp machine to reliably spray arc, you're looking at a welder from a different brand.

  3. #3
    Join Date
    Jul 2016
    Location
    Roatan island
    Posts
    71

    Re: POWER I-MIG 230I & spray transfer

    Thanks for the confirmation. It's as I suspected.

  4. #4
    Join Date
    Nov 2014
    Posts
    132

    Re: POWER I-MIG 230I & spray transfer

    According to the Miller calculator yes. BUT only up to 1/4" material. Over that you run out of voltage.

    https://www.millerwelds.com/resource...ing-calculator
    Fabricator 252i
    FP120
    Cutmaster 42
    Victor torches

  5. #5
    Join Date
    Jul 2016
    Location
    Roatan island
    Posts
    71

    Re: POWER I-MIG 230I & spray transfer

    tkevan:

    Just went to that Miller site and they want a 2% Oxygen mix ! ?
    Is that a misprint? I thought we were shielding the puddle from Oxygen by using only inert gasses like CO2 and Argon.

  6. #6
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    4,692

    Re: POWER I-MIG 230I & spray transfer

    You can use a 90/10 mix on mild steel. I personally use C 18 (82/18) on my welders and spray with it, but I don't have the 230i. The 275 units will do it fine.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  7. #7
    Join Date
    Nov 2014
    Posts
    132

    Re: POWER I-MIG 230I & spray transfer

    Quote Originally Posted by RoatanBill View Post
    tkevan:

    Just went to that Miller site and they want a 2% Oxygen mix ! ?
    Is that a misprint? I thought we were shielding the puddle from Oxygen by using only inert gasses like CO2 and Argon.
    That's a misprint. Should be 98%Argon/2% CO2. That gas with 1/4 steel puts you in the 24-25V range. Anything thicker puts you over your 25.5V.
    Fabricator 252i
    FP120
    Cutmaster 42
    Victor torches

  8. #8
    Join Date
    Nov 2008
    Location
    south GA where its hot in summer and cold in winter
    Posts
    4,692

    Re: POWER I-MIG 230I & spray transfer

    Actually, the wire diameter is going to determine when something is going to spray.
    Esab Migmaster 250
    Lincoln SA 200
    Lincoln Ranger 8
    Smith Oxy Fuel setup
    Everlast PowerPlasma 80
    Everlast Power iMIG 160
    Everlast Power iMIG 205
    Everlast Power iMIG 140E
    Everlast PowerARC 300
    Everlast PowerARC 140ST
    Everlast PowerTIG 255EXT

  9. #9
    Join Date
    Nov 2014
    Posts
    132

    Re: POWER I-MIG 230I & spray transfer

    Quote Originally Posted by lugweld View Post
    Actually, the wire diameter is going to determine when something is going to spray.
    True. The calculator gives you a ballpark voltage/IPM for .035 and .045. The 230 should hit those.
    Fabricator 252i
    FP120
    Cutmaster 42
    Victor torches

Tags for this Thread

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement