    weldanpower 225/210 6 briggs wiring diagram

    I've got a weldanpower 225/210 6 with a Briggs and no cv tap, code 8705. the wiring diagram provided by Lincoln does not match the partially destroyed diagram under the cover of my welder. specifically the idle solenoid. img 308 that Lincoln provides on their web shows the solenoid connected to taps 213 and 215 on the idler circuit board. what's left of my diagram shows the solenoid connected to taps 214 1nd 215. The rest of the diagram isn't legible and I'll need it to hook up the ignition and idle switches and ammeter without possibly doing damage to the idle or charging circuits. everything worked as it should before I disassembled for cleaning and inspection. Thanks, John

  2. #2
    Join Date
    Mar 2009
    Posts
    3,399

    Re: weldanpower 225/210 6 briggs wiring diagram

    Quote Originally Posted by jstrange View Post
    What's left of my diagram shows the solenoid connected to taps 214 and 215.
    This is all I have from my Code 8399 / no CV tap. The drawing # you're looking for is M-14140. If you can't get it done from this, I suggest emailing Lincoln and request M-14140.

    Also, the auto idle circuit will not function without the ammeter hooked up.

    Name:  w.jpg
Views: 153
Size:  188.9 KB
    "You can't out puke a buzzard"

  3. #3

    Re: weldanpower 225/210 6 briggs wiring diagram

    I appreciate the effort, that area that's burnt must be typical to this welder. My drawing is damaged in the same area . I've got my local dealer looking into finding this drawing since Lincoln has not yet responded to my request.

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,051

    Re: weldanpower 225/210 6 briggs wiring diagram

    Per P-138, unit Code# 8707 Control Wiring Diagram is M-14240 - which I don't have.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  5. #5
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,051

    Re: weldanpower 225/210 6 briggs wiring diagram

    Correction! Which I do have but is too large to post.

    Let me see if I can downsize the .pdf file.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  6. #6
    Join Date
    Mar 2009
    Posts
    3,399

    Re: weldanpower 225/210 6 briggs wiring diagram

    Quote Originally Posted by duaneb55 View Post
    Correction! Which I do have but is too large to post.

    Let me see if I can downsize the .pdf file.
    If you can't downsize the pdf, do you have the option to print it as a JPEG ?

    If not and it's the only way to get it let me know. You can email it to me and I can print it to a JPEG.

    And here's a thread where you partially explained the idler a few years back:

    http://weldingweb.com/showthread.php...51#post5948951
    "You can't out puke a buzzard"

  7. #7
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,051

    Re: weldanpower 225/210 6 briggs wiring diagram

    Here it is . . .

    M-14240.pdf


    . . . and this should be the idler board schematic . . .

    M14013.pdf
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  8. #8
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    17,051

    Re: weldanpower 225/210 6 briggs wiring diagram

    Quote Originally Posted by Pipeliner View Post
    And here's a thread where you partially explained the idler a few years back:

    http://weldingweb.com/showthread.php...51#post5948951
    Well you've got a much better memory than I.
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  9. #9

    Re: weldanpower 225/210 6 briggs wiring diagram

    I appreciate the help. i wasn't able to download the file for some reason but my local dealer was able to print off drawing M-14240, and I was back in business. was. I repaired a broken weld on a machine, shut the welder down to fab some pieces and when I started the welder up and went to weld she would spark and not weld. I found an older post here about checking the flashing diode,brushes, armature and slow blow fuse. my question regarding the flashing diode is this. when I check the diode with the fuse removed the diode measures resistance in only one direction. with the fuse installed I get a reading of 225 and rising with the ohm meter leads in the correct direction and 346 and rising in the opposite direction. as a side note, I had replaced the ignition coil recently with a new briggs electronic coil. thanks

  10. #10
    Join Date
    Mar 2009
    Posts
    3,399

    Re: weldanpower 225/210 6 briggs wiring diagram

    Name:  M-14240.jpg
Views: 82
Size:  122.5 KB

    Name:  M-14013.jpg
Views: 83
Size:  85.0 KB
    "You can't out puke a buzzard"

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement