    I've got hold of a welding/assembly table which is pretty stout with a 1" top and nearly 10' square. I'd like to get this thing cut in half to make a couple of 5X10 tables, or one 6X10, and one 4X10. I can air arc the stitch welds out to remove the horizontal tubing supports between the uprights, then need a way to slice the table lengthwise. Would a track torch do this alright? Will it deform the table top(s)? I don't have any way to use my plasma to make this long of a cut and it look good or not be jagged as hell.

    Thanks,
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  2. #2
    Join Date
    Apr 2006
    Location
    Outside of Raleigh, NC
    Posts
    600

    Re: Ned to cut a welding table down:

    It would be slow going but I've cut 1" plate with an evolution saw.
    Miller Trailblazer Pro 350D
    Miller Suitcase MIG
    Miller Spectrum 2050
    Miller Syncrowave 250DX
    Lincoln 210MP

  3. #3
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    2,432

    Re: Ned to cut a welding table down:

    I just cut a little 1" plate with my 8" Milwaukee. Pack a lunch...and two blades.

  4. #4
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,860

    Re: Ned to cut a welding table down:

    Torch and straightedge. Get the right size tip and have at it. Be sure to tack in some supports to prevent sagging. I have the Milwaukee saw and would only use it as a last resort, as you will probably burn it up and go thru a small fortune in blades.

  5. #5
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,839

    Re: Ned to cut a welding table down:

    Thanks for the suggestions so far. I can borrow a track torch and I'm wondering if my PM-85 rigged up to it running slow would do the job? I know the track torch itself would do it but I'm concerned about warping on the cut edge. The table is blanchard ground and I really don't want to distort it although I really don't require that precision.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  6. #6
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,054

    Re: Ned to cut a welding table down:

    I would use a track torch. Fastest way to go!
    Attached Images Attached Images  
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  7. #7
    Join Date
    Apr 2011
    Location
    minnesota
    Posts
    1,910

    Re: Ned to cut a welding table down:

    Plasma would work with a good straight edge and a keen eye
    Millermatic 252
    millermatic 175
    miller 300 Thunderbolt
    lincoln ranger 250
    smith torches
    lots of bfh's
    If it dont fit get a bigger hammer

  8. #8
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    2,432

    Re: Ned to cut a welding table down:

    Quote Originally Posted by farmshop View Post
    Plasma would work with a good straight edge and a keen eye
    And a MAN air compressor. I guess my 65 would do it with my 7.5 Copco. I'd still use my Milwaukee as first choice.A track torch is a gem but not many people choose this as a "hobby" any more. That's when the Plasma cutter( even an 85) becomes a toy and those two tanks tell it to step aside and "hold my beer".I'm pretty good with a flat bar and an O/A torch but on over 1/2 inch thick---------nnnnnnnnnnnnnn. Gimme a track torch.
    HMMMMMMMMm I do have a Hypethermic magnetic circle cutter with training wheels. Maybe I should take a shot at some 1" tomorrow. I need to raise the jack in my press brake another couple inches.
    Last edited by Bonzoo; 08-09-2017 at 08:54 PM.

  9. #9
    Join Date
    Apr 2006
    Location
    Western, NY
    Posts
    235

    Re: Ned to cut a welding table down:

    If you get the right tip. A track torch will give you a cut that will look like it is sawed. It takes a little practice, I don't think that plate will bow sideways. That would be your biggest worry useing a torch. Vertically you can always clamp a stiffener to it to keep that true. Although I don't think it will move in that direction.

  10. #10
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,839

    Re: Ned to cut a welding table down:

    This table has nine legs under it and all are adjustable for elevation. I will relocate the inner legs, (stitch welded) and remove the very center one to appropriate positions for new perimeter tubes to tie into. I will be leaving a 2.25" inch gap between the new center tubes, (these will be the new perimeter tubes of the smaller tables) they will run the torch centered between these tubes severing the table. They have a lot of experience with their track torch and 1", and 1.25" plate cutting with it. I will supply the gasses and they will set it up in my shop and do the cut.

    Thanks for the assist.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  11. #11
    Join Date
    Mar 2016
    Location
    Minneapolis MN
    Posts
    579

    Re: Ned to cut a welding table down:

    Wondering if the torch heat will warp the table top?

  12. #12
    Join Date
    May 2010
    Location
    Port Orchard, WA.
    Posts
    10,054

    Re: Ned to cut a welding table down:

    Quote Originally Posted by cloudman View Post
    Wondering if the torch heat will warp the table top?
    If torch heat can warp it. Torch heat, and a little water can fix it too.
    Don’t pay any attention to me
    I’m just a hobbyist!

    Carl

    Dynasty 300
    V350-Pro w/pulse
    SG Spool gun
    1937 IdealArc-300
    PowerArc 200ST
    3 SA-200s
    Vantage 400





  13. #13
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,839

    Re: Ned to cut a welding table down:

    Got a call from a gent whom knows another buddy of mine I was discussing a track torch and this table with. Guess I now own one of these things as a gift w/12' of track, extra tips, hose and working knowledge to get me started. The unit was replaced with a plasma table and sits unused.

    Think ole Slob needs to get the guy a complimentary case of beer no?
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  14. #14
    Join Date
    Nov 2012
    Location
    pittsburgh,pa.
    Posts
    112

    Re: Ned to cut a welding table down:

    Nice!Maybe a couple of steak's too!
    either you LIKE BACON or you're WRONG!!!! "There are three kinds of men.The ones that learn by readin'.The few who learn by observation.The rest of them have to pee on the electric fence for themselves"-Will Rogers

  15. #15
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,860

    Re: Ned to cut a welding table down:

    Once you get the track setup dialed in you should have no problems with warpage. Your cut will spread open quite a bit as your cutting so prepare for that. The spreading is actually a good thing as that will help prevent warping. Should work out good for that and it might be worth adapting plasma to the buggy for use down the road. Good luck with the table.

  16. #16
    Join Date
    Jun 2016
    Location
    Not there
    Posts
    2,432

    Re: Ned to cut a welding table down:

    Quote Originally Posted by cloudman View Post
    Wondering if the torch heat will warp the table top?
    Not as bad as a crappy shear with a dull blade or a 'tard on a forklift but yeah, a little. Like CEP says. A lil heat can fix it right quick.

  17. #17
    Join Date
    Oct 2006
    Location
    Illinois
    Posts
    8,893

    Re: Ned to cut a welding table down:

    I think I would sell it for big $$$ and build new to your needs.

  18. #18
    Join Date
    Oct 2016
    Posts
    57

    Re: Ned to cut a welding table down:

    How about score it 1/4 deep on one or both sides, then only have to torch or plasma through less thickness with less warpage?

  19. #19
    Join Date
    Mar 2009
    Posts
    3,393

    Re: Ned to cut a welding table down:

    I would pony up for some scrap 1" plate to test your track torch on before going at the big piece. You can practice and see what settings you need for the torch and speed.
    "You can't out puke a buzzard"

  20. #20
    Join Date
    Oct 2011
    Location
    Jacksonville Florida
    Posts
    2,391

    Re: Ned to cut a welding table down:

    Tack a straight edge to it and cut with O/A. You should be done by now... A grinder will clean up the edge.
    Airco Ac/Dc 300 Heliwelder
    MillerMatic 200
    Miller Maxstar 150STL

  21. #21
    Join Date
    Nov 2014
    Location
    PDX Pacific NW
    Posts
    7,381

    Re: Ned to cut a welding table down:

    My bench was cut with a track torch and it's within 1/32 over 8' and nice and straight still. Paid 55 cents a pound for it. Need a new one since it's warped now

  22. #22
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,839

    Re: Ned to cut a welding table down:

    Was talking to another gent whom knows a friend someplace in Texas whom has a 5X10 cast iron welding table for sale. I guess this thing has several "T" slots that take hold down clamps like a milling machine would use. What would be the benefit to a cast iron table other than very stiff?
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

  23. #23
    Join Date
    Sep 2013
    Location
    central Wis.
    Posts
    3,860

    Re: Ned to cut a welding table down:

    Quote Originally Posted by Slob View Post
    Was talking to another gent whom knows a friend someplace in Texas whom has a 5X10 cast iron welding table for sale. I guess this thing has several "T" slots that take hold down clamps like a milling machine would use. What would be the benefit to a cast iron table other than very stiff?
    It would be much more rigid, pound for pound than mild steel. Usually something like that in cast iron would have lots of stiffener webbing and be thinner overall. The down side is tacking fixtures or parts to the table isn't practical.

  24. #24
    Join Date
    Jul 2017
    Location
    Florida
    Posts
    88

    Re: Ned to cut a welding table down:

    Know anybody with a flatbed or trailer, BA forklift and a water jet?

    0 warpage.
    HTP 221 water cooled

  25. #25
    Join Date
    Jul 2014
    Location
    Bulldog Heaven at the end of my chain
    Posts
    2,839

    Re: Ned to cut a welding table down:

    The track torch showed up at the shop today. Cost me about $14.00 for breakfast at the truck stop but still don't think I did too bad.

    Everything works as it should with the exception of needing some cleaning and lubrication to make things smooth. Teeth all look good and it uses "Victor" cutting tips. The speed is very linear and adjustable fore and aft, along with the clutch working well.

    Can't attach photos tonight for some reason; maybe later.
    Slob

    Purveyor of intimate unparalleled knowledge of nothing about everything.

    Oh yeah, also an unabashed internet "Troll" too.....

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement