    How does a Helium / Argon MIX stay mixed?

    Argon is one of the heaviest gasses. Helium is one of the lightest. They wouldn't mix out of the bottle (think of the lengths we go to when backing up a weld with argon). So how are they a mixture in a bottle? Surely the take-off valve at the top sucks the helium first? Or is there something i don't know about the bottles it comes in?
    Likes long walks in the dark & late nights by the fire with a good whine. Down to earth and easy flowing. Polished appearance. Into lots of pre-heating & satisfying the puddle. Seeks firey weld with long legs, overlapping toes, and small ripples.

  2. #2
    Join Date
    Mar 2005
    Location
    Under a Rock
    Posts
    3,135

    Re: How does a Helium / Argon MIX stay mixed?

    How does the air we breath stay mixed?

    ponder...
    Miller 211/Spoolmate 100
    1961 Lincoln Idealarc 250
    Hypertherm PM 45
    Lincoln SP125 plus
    HTP 221
    Chicom spot welder



    True Wisdom only comes from Pain.

  3. #3
    Join Date
    Mar 2015
    Location
    South Africa, KwaZulu-Natal.
    Posts
    76

    Re: How does a Helium / Argon MIX stay mixed?

    Okay, I looked into it a bit. (Following a lead in a comment by Fred S in another thread, about the entropy of mixing.)
    The reason that it _seems_ to be that they would separate is because of a (my) poor understanding of what mixing means. It's not about combining, aggitating, or stirring things that want to be apart. More like a physics thing, with ideal gas laws etc. In fact that impetus to be separate because of one being lighter actually doesn't factor into it.
    The absolute simplest explanation is that once they're mixed, it would take energy to separate them, and there's nowhere that energy is coming from.
    The next level explanation involves imagining opening a valve between bottles of argon and helium. Soon as you do, there's 'new' room for the argon in the helium bottle, and 'new' room for helium in the argon bottle, so they spread out to occupy that space. And it would take 'convincing' to get all the atoms of one gas to squeeze back into only one bottle, or indeed one section of a closed system (important to remember it's a closed system and the rules are different). Gravity just doesn't have that kind of energy. It can slow things from mixing when out of a bottle. But once mixed inside a bottle there's no going back.
    Likes long walks in the dark & late nights by the fire with a good whine. Down to earth and easy flowing. Polished appearance. Into lots of pre-heating & satisfying the puddle. Seeks firey weld with long legs, overlapping toes, and small ripples.

  4. #4
    Join Date
    May 2008
    Location
    Orange, TX
    Posts
    16,609

    Re: How does a Helium / Argon MIX stay mixed?



    You nailed it. It's not like water and oil that naturally repel each other but as you discovered they are "mixed" to begin with and must be separated "by force".


    I was going to say because the guy filling the cylinder tells them to but . . .
    MM200 w/Spoolmatic 1
    Syncrowave 180SD
    Bobcat 225G Plus - LP/NG
    MUTT Suitcase Wirefeeder
    WC-1S/Spoolmatic 1
    HF-251D-1
    PakMaster 100XL
    '68 Red Face Code #6633 project
    Star Jet 21-110

    Save 2nd Base!

  5. #5
    Join Date
    Jan 2016
    Posts
    2,612

    Re: How does a Helium / Argon MIX stay mixed?

    Quote Originally Posted by Reseda luteola View Post
    Argon is one of the heaviest gasses. Helium is one of the lightest. They wouldn't mix out of the bottle (think of the lengths we go to when backing up a weld with argon). So how are they a mixture in a bottle? Surely the take-off valve at the top sucks the helium first? Or is there something i don't know about the bottles it comes in?
    just shake the cylinder before use, all the ones on the welding trucks get mixed as they drive and hit bumps..........................yeah that sounds good..

  6. #6
    Join Date
    Feb 2005
    Location
    Louisiana
    Posts
    1,923

    Re: How does a Helium / Argon MIX stay mixed?

    Quote Originally Posted by Hobbytime View Post
    just shake the cylinder before use, all the ones on the welding trucks get mixed as they drive and hit bumps..........................yeah that sounds good..
    Either that or just roll them around on the shop floor to remix the gases!

  7. #7
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,000

    Re: How does a Helium / Argon MIX stay mixed?

    There is a LOT of empty space between molecules. They bop around amongst themselves and never notice the other guys. Compress them to about the density of people living in Hong Kong and you might see some action.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  8. #8
    Join Date
    Nov 2014
    Posts
    31

    Re: How does a Helium / Argon MIX stay mixed?

    Quote Originally Posted by Reseda luteola View Post
    The absolute simplest explanation is that once they're mixed, it would take energy to separate them, and there's nowhere that energy is coming from.
    Unfortunately, that is completely wrong. There is a lot of energy in the system, with the energy of each atom a constant times the absolute temperature (room temperature is approximately 300 Kelvin).

    This thermal energy results in the argon atoms moving at nearly 1000 mph, and the helium atoms moving ~2.5x faster. Although gravity acts on both types of atoms, the force of gravity is weak compared with this thermal energy. Under the effect of gravity alone the argon would sink to the bottom of the bottle because it is heavier than helium and the gravitational force is proportional to mass. However, each argon (and helium) atom is bombarded by 1000 mph argon atoms (and 2500 mph helium atoms) that hit it from all sides so frequently that it only moves a few micro-inches after a hit before it's hit again. Since the forces from those constant, random impacts is so much larger than that of gravity the atoms remain mixed.

  9. #9
    Join Date
    Oct 2003
    Location
    The armpit of Portland.
    Posts
    1,410

    Re: How does a Helium / Argon MIX stay mixed?

    Quote Originally Posted by MCTig View Post
    ...atom is bombarded by 1000 mph argon atoms (and 2500 mph helium atoms) that hit it from all sides so frequently that it only moves a few micro-inches after a hit before it's hit again. Since the forces from those constant, random impacts is so much larger than that of gravity the atoms remain mixed.
    That statement makes me think that the gas would never cool down after being compressed.
    Common sense in an uncommon degree is what the world calls wisdom.

  10. #10
    Join Date
    Nov 2008
    Location
    Texas Near Dallas
    Posts
    1,082

    Re: How does a Helium / Argon MIX stay mixed?

    Quote Originally Posted by Brainfarth View Post
    That statement makes me think that the gas would never cool down after being compressed.
    The gases are moving that fast because they're at room temperature. When they're compressed and heated they're moving even faster!!! When they hit the sides of the relatively cold container, they give off more heat than they receive (bounce back with less speed). Eventually they'll slow down to the speeds at room temperature.

    Dynasty200DX w/coolmate1
    MM210
    MM Vintage
    ESAB miniarc161lts
    Lincoln AC225
    Victor O/A, Smith AW1A
    Cutmaster 81
    IR 2475N7.5FP
    Rage3
    Jancy USA101
    9" SB
    AEAD-200LE

  11. #11
    Join Date
    Mar 2004
    Location
    B.C. Canada
    Posts
    2,679

    Re: How does a Helium / Argon MIX stay mixed?

    It seems I managed to pay attention in grade eight when "Brownian motion" was explained. As a result my little mind never worries about gases mixing.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement