    Quote Originally Posted by gxbxc View Post
    if you are able ,mix up some epoxy and pour it into the picket hole after you install the pickets , it will sure tighten them up
    That is very effective, I have done that on several jobs. It is very high strength. I would compare it to Quick-Rock in a cored hole in a cement stoop.


    Name:  cap3.jpg
Views: 125
Size:  75.0 KB

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  2. #27

    Re: Stair handrail with no bottom rail

    They used to put a screw on an angle into the floor and then drop a little square escutcheon over it.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  3. #28
    Join Date
    Mar 2016
    Location
    Minneapolis MN
    Posts
    579

    Re: Stair handrail with no bottom rail

    cool metalman, post the finished product when your done - hopefully another portfolio piece!

  4. #29
    Join Date
    Jun 2012
    Location
    CT
    Posts
    2,134

    Re: Stair handrail with no bottom rail

    Quote Originally Posted by gxbxc View Post
    if you are able ,mix up some epoxy and pour it into the picket hole after you install the pickets , it will sure tighten them up
    Yes I was thinking about this, I might do it

    Sent from my SM-J327T using Tapatalk

  5. #30
    Join Date
    Jun 2012
    Location
    CT
    Posts
    2,134

    Re: Stair handrail with no bottom rail

    I made a sample, they loved it, so it's a go https://uploads.tapatalk-cdn.com/201...75dd89416e.jpg

    Sent from my SM-J327T using Tapatalk

  6. #31
    Join Date
    Jun 2012
    Location
    Bemidji MN
    Posts
    13,812

    Re: Stair handrail with no bottom rail

    That looks really nice
    Dave J.

    Beware of false knowledge; it is more dangerous than ignorance. ~George Bernard Shaw~

    Airco 300 - Syncro 350
    Invertec v250-s
    Thermal Arc 161 and 300
    MM210
    Dialarc
    Tried being normal once, didn't take....I think it was a Tuesday.

  7. #32

    Re: Stair handrail with no bottom rail

    Quote Originally Posted by MetalMan23 View Post
    I made a sample, they loved it, so it's a go https://uploads.tapatalk-cdn.com/201...75dd89416e.jpg

    Sent from my SM-J327T using Tapatalk
    Looks really good.

    Sincerely,

    William McCormick
    If I wasn't so.....crazy, I wouldn't try to act normal, and you would be afraid.

  8. #33
    Join Date
    Jun 2012
    Location
    CT
    Posts
    2,134

    Re: Stair handrail with no bottom rail

    Thanks guys, I'm making the first couple of sections and we'll install them end of next week

    Sent from my SM-J327T using Tapatalk

  9. #34
    Join Date
    Jul 2008
    Location
    Long Island
    Posts
    2,846

    Re: Stair handrail with no bottom rail

    I can't wait to see it. So far, it looks beautiful, though it also looks like a lot of extra work.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement