    TIG 175 squarewave

    Looking at a used machine. Will this tig weld aluminum up to 3/16? How thick steel will it right and stick weld. Thanks

  2. #2
    Join Date
    Feb 2014
    Location
    n.w. of chicago
    Posts
    695

    Re: TIG 175 squarewave

    .175 thick general rule 1 amp per thousandth of inch, duty cycle could be a issue depending on what your doing but it's a nice machine that will / should last a long time for most motorsport around house small fab work should be fine it really is a nice welder

  3. #3
    Join Date
    Nov 2009
    Location
    Seward, Ak
    Posts
    284

    Re: TIG 175 squarewave

    So you are saying it will manage the material thickness but the duty cycle may make a large job a long slow process?

  4. #4
    Join Date
    Feb 2014
    Location
    n.w. of chicago
    Posts
    695

    Re: TIG 175 squarewave

    Pretty much If it's going to be fed a steady diet of .187 aluminum I would look for a 250 class machine occasionally welding up there it should be fine duty cycle is funky anyway alot of times if it's cooler out your duty cycle goes up I think they rate them at 104f for stick it probably be fine 3/32 1/8 7018 maybe around 70 - 110 amps weld til your bored

  5. #5
    Join Date
    Jan 2004
    Posts
    1,598

    Re: TIG 175 squarewave

    For hobbyist level use, in stick mode, one inch thick steel shouldn't be a problem as long as the operator skill level is up to the task.

    On AC TIG to use all 175 amps, is going to require more than a 50 amp input circuit. At work the 50 amp breaker was tripping all the time. Asked for a 70 amp circuit. Got a 90 amp circuit instead. Never had a breaker tripping issue with the 90 amp circuit.

    I am not fond of the Auto-balance, it tends to want to ball the tungsten severely. The adjustable balance that Lincoln added to the Precision TIG 225 makes it a nicer aluminum unit.

    It doesn't bother me, but I'll point out that the post flow is a fixed 15 seconds.
    ESAB Migmaster 250
    Hobart Ironman 230
    TWECO Fabricator 181i & 211i
    Multimatic 215
    Handler 125EZ


    Maxstar 150 STH - very nice

  6. #6
    Join Date
    Feb 2009
    Location
    Chicago
    Posts
    6,605

    Re: TIG 175 squarewave

    I bet that machine may struggle a little bit at 3/16"
    Torchmate 2x2 CNC with Flashcut CNC controls
    Hypertherm Powermax45
    2015 AHP Tig
    CK Tig Welder
    Razorweld 200ac/dc Tig
    RazorMig 180 & Spoolgun
    Vipercut 30 Plasma
    Razorweld, SSC Foot Pedal & MK Products & Atlas & MBC Dealer and more

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement