    Lincoln SP135 T with 0.023"

    Hello guys

    This is my first post since I am new in the forum and welding as well.
    I got a 2.2 pounds 0.23" ER70S-6 spool to use with my also new Lincoln SP135T, but as far I can see my machine works with 0.025 to 0.035 wires although the manual said "The SP-135T is shipped from the factory ready to feed .023”-.025” (0.6 mm) diameter wire ".
    Can I use the 0.023" wire if so what should I expect for. I am in a very tight budget to loose money so help me find out if this wire could work

    Thanks in advance

  2. #2
    Join Date
    Sep 2008
    Location
    Dalton, GA
    Posts
    1,531

    Re: Lincoln SP135 T with 0.023"

    .023 is the same as .025. Some manufacturers call it one and some call it the other. Just set up according to the manual for .025.

    Be sure to check polarity to match the wire with gas.

    Then just start practicing.

    Welcome to the forum.
    Burt
    _____________________
    Miller Syncrowave 250
    Millermatic 211 w/Spoolmate
    Miller 375 Plasma Cutter
    Miller Thunderbolt XL AC/DC
    10FtDrillBit.com

  3. #3
    Join Date
    Feb 2017
    Posts
    170

    Re: Lincoln SP135 T with 0.023"

    I have an SP135+ and use. 023 wire exclusively in it. It works just fine. Just be sure you have the feed rollers set up the right way, otherwise it will slip.
    Home tinkerer and old tool junkie

    Lincoln SP 135 Plus
    Ĺincoln Idealarc 250/250
    AHP AlphaTIG 200
    Viper Cut 30 Plasma
    Harris O/A Port-A-Torch
    Coal forge & anvil

  4. #4
    Join Date
    Sep 2017
    Location
    Caracas, Venezuela
    Posts
    4

    Re: Lincoln SP135 T with 0.023"

    Thank you guys I will let you know how the .023" works on the machine, if the weld does not go right should be my fault hahaha

  5. #5
    Join Date
    May 2006
    Location
    Northern California
    Posts
    1,854

    Re: Lincoln SP135 T with 0.023"

    .023 is fine for either the SP135 or theSP175+ that I gave to my son. It's a good all around wire for that size of machine.
    Miller Millermatic 252
    Miller Syncrowave 200
    Liincoln AC-DC 225
    Victor O-A Set

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement