    Re: Crack repair using 312 stainless rods

    One definition of insanity is doing the same thing over and over expecting a different result. It sounds like you are responsible for performing someone else's insanity.

  2. #27
    Join Date
    Jul 2017
    Posts
    179

    Re: Crack repair using 312 stainless rods

    It's look similar for heat exchanger..
    Last edited by mohdnawi838; 11-14-2017 at 11:06 AM.

  3. #28
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,518

    Re: Crack repair using 312 stainless rods

    In the 2nd pic in post #19 it appears the crack formed where the elbow joins the main assy. If the left end of the straight pipe is anchored solidly could the crack be due to linear expansion of the straight section causing the crack to form in that area? If so maybe installing a stainless flex coupling in the straight pipe would relieve the stress.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Hobart G-213
    Victor O/A setup
    Makita chop saw

  4. #29
    Join Date
    Jul 2017
    Posts
    135

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by bent View Post
    One definition of insanity is doing the same thing over and over expecting a different result. It sounds like you are responsible for performing someone else's insanity.
    This is what I was saying from the beginning as well. And the 0P agrees with us. You know how foreman are though. Simply reading the word shut down makes them break out in a cold sweat while browsing through a dictionary. It is the world we live in.


    Everlast PowerMTS221 sti

  5. #30
    Join Date
    Jan 2017
    Posts
    41

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by mohdnawi838 View Post
    What about P91?

    Just opinion..
    Purely a cost decision, the elbow pictured is $13grand shipped to your door from china, using an alloy like p91 or inconel would push that price up 50x.

  6. #31
    Join Date
    Jul 2017
    Posts
    135

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by Hayden View Post
    Purely a cost decision, the elbow pictured is $13grand shipped to your door from china, using an alloy like p91 or inconel would push that price up 50x.
    Do you have a rough ETA on when we will be getting to see the gorgeous repair work?



    Everlast PowerMTS221 sti

  7. #32
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,894

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by Hayden View Post
    Purely a cost decision, the elbow pictured is $13grand shipped to your door from china, using an alloy like p91 or inconel would push that price up 50x.
    Is that a production item? $13K is dirt cheap. What is the wall thickness again?
    Weld like a "WELDOR", not a wel-"DERR"
    Miller Dynasty700DX, Dynasty350DX 2ea., Dynasty200DX, ThermalArc 400 GTSW, LincolnSW200 2ea., MillerMatic350P, MillerMatic200 with spoolgun, MKCobraMig260, Lincoln SP-170T,PlasmaCam/Hypertherm 1250

  8. #33
    Join Date
    Jan 2017
    Posts
    41

    Re: Crack repair using 312 stainless rods

    No there not production items, its just chinese manufacturing mate
    Attached Images Attached Images   

  9. #34
    Join Date
    Jul 2017
    Posts
    135

    Re: Crack repair using 312 stainless rods

    Damn man that looks like a blast!


    Everlast PowerMTS221 sti

  10. #35
    Join Date
    Jan 2017
    Posts
    41

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by aaronUSMC View Post
    Damn man that looks like a blast!


    Everlast PowerMTS221 sti
    Take my word for it, it isnt...

  11. #36
    Join Date
    Jul 2017
    Posts
    179

    Re: Crack repair using 312 stainless rods

    I believe material it self can't handle the pressure and heat

  12. #37
    Join Date
    Dec 2010
    Location
    SoCal-LA
    Posts
    8,894

    Re: Crack repair using 312 stainless rods

    Let me get this straight. You are repairing ruptures in the pipe walls, or the original welds joining the pipes?
    Weld like a "WELDOR", not a wel-"DERR"
    Miller Dynasty700DX, Dynasty350DX 2ea., Dynasty200DX, ThermalArc 400 GTSW, LincolnSW200 2ea., MillerMatic350P, MillerMatic200 with spoolgun, MKCobraMig260, Lincoln SP-170T,PlasmaCam/Hypertherm 1250

  13. #38
    Join Date
    Jan 2017
    Posts
    41

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by shovelon View Post
    Let me get this straight. You are repairing ruptures in the pipe walls, or the original welds joining the pipes?

    "Ruptures" or cracks... Yes, the repairs are always in the run of pipe not in the returns that join them together. General consensus seems to be that they are due to creep stresses in the material aka metal fatigue

  14. #39
    Join Date
    Jul 2017
    Posts
    135

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by Hayden View Post
    Take my word for it, it isnt...
    Complete and total sarcasm on my part. I feel for you right now.


    Everlast PowerMTS221 sti

  15. #40
    Join Date
    Apr 2006
    Location
    Soda springs,Id
    Posts
    4,518

    Re: Crack repair using 312 stainless rods

    Don't know the age of this unit. Maybe it's time to shell out another $13k.
    Mike
    Ol' Stonebreaker
    "Experience is the name everyone gives to their mistakes"

    Miller 175 mig
    Miller thunderbolt ac/dc stick
    Hobart G-213
    Victor O/A setup
    Makita chop saw

  16. #41
    Join Date
    Jul 2017
    Posts
    135

    Re: Crack repair using 312 stainless rods

    Any updates on the situation?


    Everlast PowerMTS221 sti

  17. #42
    Join Date
    Jan 2017
    Posts
    41

    Re: Crack repair using 312 stainless rods

    Quote Originally Posted by aaronUSMC View Post
    Any updates on the situation?


    Everlast PowerMTS221 sti

    Still early days brother, will keep you posted.

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement