    Is Delrin/acetal the best choice for this?

    I'm looking to build a roll bender for 7/8" to 1" aluminum and stainless tube. Similar to the one included.
    I will probably make the dies out of plywood initially to test it out. To replace them, I was looking at using a piece of 3" round bar acetal. Will this work or will it be too slippery? Anything else that would work better? I'm thinking that with the pressure from the top roller, it will bite in enough to prevent slipping.

    Name:  PICT0042.jpg
Views: 368
Size:  66.5 KB
    Campbell Hausfeld Fluxcore 80
    Thermal Arc 185
    Millermatic 250
    JD Squared model 32 bender

  2. #2
    Join Date
    Mar 2007
    Location
    Lookout, West Virginia
    Posts
    184

    Re: Is Delrin/acetal the best choice for this?

    It will probably slip more on the SS than the AL, but as long as you aren't bending it too much with each pass, it might work. You can always just shove the tube through while the other hand turns the crank.

  3. #3
    Join Date
    Jan 2008
    Location
    Richmond, Virginia
    Posts
    7,065

    Re: Is Delrin/acetal the best choice for this?

    Aluminum dies for the geared rollers would have more grip.
    "USMCPOP" First-born son: KIA Iraq 1/26/05
    Syncrowave 250 w/ Coolmate 3
    Dialarc 250, Idealarc 250
    SP-175 +
    Firepower TIG 160S (gave the TA 161 STL to the son)
    Lincwelder AC180C (1952)
    Victor & Smith O/A torches
    Miller spot welder

  4. #4
    Join Date
    Jan 2011
    Location
    Hutchinson Kansas
    Posts
    463

    Re: Is Delrin/acetal the best choice for this?

    Gears would also work better than sprockets
    Lincolin Power Wave 450, Lincoln Powermig 255, Lincoln Pro Mig 140, Lincoln Squarewave Tig 275, Miller Big 40 G(with Hobart Hefty suitcase), Thermal Arc 95S and Esab PCM875 in an already full machine shop.

  5. #5
    Join Date
    Mar 2006
    Posts
    60

    Re: Is Delrin/acetal the best choice for this?

    Quote Originally Posted by Oldendum View Post
    Aluminum dies for the geared rollers would have more grip.
    Both the aluminum (anodized) and stainless will be polished and have to avoid scratching it.
    Campbell Hausfeld Fluxcore 80
    Thermal Arc 185
    Millermatic 250
    JD Squared model 32 bender

  6. #6
    Join Date
    Mar 2006
    Posts
    60

    Re: Is Delrin/acetal the best choice for this?

    Quote Originally Posted by propanehotrod View Post
    Gears would also work better than sprockets
    I think so too. I'm looking to try to find some. I think the reason for the sprockets is because the dies are slippery to give it double to bite.
    Campbell Hausfeld Fluxcore 80
    Thermal Arc 185
    Millermatic 250
    JD Squared model 32 bender

  7. #7
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,113

    Re: Is Delrin/acetal the best choice for this?

    If not cost prohibitive, then you might consider dissecting a HF planetary ring roller. I suspect slipping will be more prevalent the tighter your radius. My small hf roller has no knurling left and only slips if I roll real tight.

  8. #8
    Join Date
    May 2010
    Location
    ct.
    Posts
    934

    Re: Is Delrin/acetal the best choice for this?

    Delrin is fairly slippery stuff.
    Maybe not so good where traction is necessary.
    Miller a/c-d/c Thunderbolt XL
    Millermatic 180
    Purox O/A
    Smith Littletorch O/A

    Vintage-
    -South Bend 9in. lathe
    -South Bend 7in. shaper
    -Craftsman power hacksaw
    -FibreMetal 710
    -B&D mag drill
    Cheapo-
    - Chinese mill/drill

  9. #9
    Join Date
    Jan 2011
    Location
    W. Wisc
    Posts
    317

    Re: Is Delrin/acetal the best choice for this?

    What about a urethane or rubber coating on a steel wheel? You would get good grip and no-marring surface that way. Depends how serious you are about this. There are places that can coat rollers like this, but it will cost. I suspect Delrin or any plastic is going to be too slick.
    -Dave
    XMT304, 22A Feeder, HF251D Hi Freq box

  10. #10
    Join Date
    May 2014
    Location
    Manitoba Canada
    Posts
    1,675

    Re: Is Delrin/acetal the best choice for this?

    Would a small diameter wide rubber band in each roller help?
    F-225 amp Forney AC Stick
    230 amp Sears AC Stick
    Lincoln 180C MIG
    Victor Medalist 350 O/A

  11. #11
    Join Date
    Mar 2006
    Posts
    60

    Re: Is Delrin/acetal the best choice for this?

    Quote Originally Posted by whtbaron View Post
    Would a small diameter wide rubber band in each roller help?
    Not a bad idea. I was thinking about gluing a piece of rubber on a plywood die initially to test it out.
    Campbell Hausfeld Fluxcore 80
    Thermal Arc 185
    Millermatic 250
    JD Squared model 32 bender

  12. #12
    Join Date
    Mar 2006
    Posts
    60

    Re: Is Delrin/acetal the best choice for this?

    Quote Originally Posted by davec View Post
    What about a urethane or rubber coating on a steel wheel? You would get good grip and no-marring surface that way. Depends how serious you are about this. There are places that can coat rollers like this, but it will cost. I suspect Delrin or any plastic is going to be too slick.
    Definitely something I will look into when I get the design figured out. Thanks
    Campbell Hausfeld Fluxcore 80
    Thermal Arc 185
    Millermatic 250
    JD Squared model 32 bender

  13. #13

    Re: Is Delrin/acetal the best choice for this?

    Cut a piece of truck inner tube and glue it to the rollers with something like 3M super weatherstrip adhesive. The tube will be thick enough to protect the surface and provide grip at the same time.

    Sent from my hammer and chisel using Tapatalk

  14. #14
    Join Date
    Nov 2005
    Location
    Nashville, TN
    Posts
    3,113

    Re: Is Delrin/acetal the best choice for this?

    How does the roller in the photo perform?

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement