    Victor Kwik Connect

    so as far as I understand Victor and ESAB are a combined company? maybe someone on here will know/let me know... on the Victor Torch to hose Kwik Connects is there any way to buy just the "male" fitting that I can put on all my torches and not have to keep buy the sets? I called Victor/ESAB and the customer service person had not idea.. part number of the set is 0656-0000 thank you

  2. #2
    Join Date
    Mar 2010
    Location
    Ceres, California
    Posts
    3,371

    Re: Victor Kwik Connect

    Customer service is clue less. Call tech support for these type of questions.

  3. #3
    Join Date
    Jul 2016
    Location
    Midwest
    Posts
    224

    Re: Victor Kwik Connect

    Probably not, I believe they are sets only. You can easily get them individually from Koike. Much better product and no suffering from ESAB Lack of customer service.

  4. #4
    Join Date
    Jan 2011
    Location
    Hutchinson Kansas
    Posts
    472

    Re: Victor Kwik Connect

    I posted about this a while back
    http://weldingweb.com/showthread.php...+quick+connect
    I see they have added hose barb quick connectors recently too.
    http://www.ibeda.com/en/gas-quick-ac...plings-iso7289
    Lincolin Power Wave 450, Lincoln Powermig 255, Lincoln Pro Mig 140, Lincoln Squarewave Tig 275, Miller Big 40 G(with Hobart Hefty suitcase), Thermal Arc 95S and Esab PCM875 in an already full machine shop.

  5. #5
    Join Date
    Feb 2016
    Location
    Ny
    Posts
    40

    Re: Victor Kwik Connect

    Quote Originally Posted by ccawgc View Post
    Customer service is clue less. Call tech support for these type of questions.
    thats what I meant, it was a good hour long conversation about the "kwik connects" and probably 40 mins explaining their product to them, then the fact that I didn't want a set just for the oxygen side or acetylene side, then the confusion about calling the male connector a male bc it has female 9/16x18 tpi, so after all that was sorted out the very unassuring answer was "no....I don't think so"


    Quote Originally Posted by Rondo View Post
    Probably not, I believe they are sets only. You can easily get them individually from Koike. Much better product and no suffering from ESAB Lack of customer service.
    so then I looked into Koike and found I can buy each piece individually, although the only place I found them online was fastenal (any one have a better source?) but I just wanted to make one more final attempt before selling them and going to Koike.

  6. #6
    Join Date
    Feb 2016
    Location
    Ny
    Posts
    40

    Re: Victor Kwik Connect

    Quote Originally Posted by propanehotrod View Post
    I posted about this a while back
    http://weldingweb.com/showthread.php...+quick+connect
    I see they have added hose barb quick connectors recently too.
    http://www.ibeda.com/en/gas-quick-ac...plings-iso7289

    as a Machinist/welder I like those a lot. they look very well made... any idea on where I can find them on the computer?

  7. #7
    Join Date
    Jan 2011
    Location
    Hutchinson Kansas
    Posts
    472

    Re: Victor Kwik Connect

    http://oxyfuelsafety.com/quick-connectors
    Here is the catalog. look at pages 6-8
    http://oxyfuelsafety.com/virteom/upl...1400077092.pdf
    I used the catalog to get a list of part #'s then called airgas and had them place the order.

    I just realized this is an esab sponsored thread. Sorry esab. I didn't mean to poke you in the eye, but I do think these are superior quick connects
    Lincolin Power Wave 450, Lincoln Powermig 255, Lincoln Pro Mig 140, Lincoln Squarewave Tig 275, Miller Big 40 G(with Hobart Hefty suitcase), Thermal Arc 95S and Esab PCM875 in an already full machine shop.

  8. #8
    Join Date
    Feb 2016
    Location
    Ny
    Posts
    40

    Re: Victor Kwik Connect

    Quote Originally Posted by propanehotrod View Post
    http://oxyfuelsafety.com/quick-connectors
    Here is the catalog. look at pages 6-8
    http://oxyfuelsafety.com/virteom/upl...1400077092.pdf
    I used the catalog to get a list of part #'s then called airgas and had them place the order.

    I just realized this is an esab sponsored thread. Sorry esab. I didn't mean to poke you in the eye, but I do think these are superior quick connects



    I wouldn't feel bad, they don't even seem to monitor there thread...

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •  
RSS | Home | Penton Media | Contact Us | Subscribe | For Advertisers | Terms of Use | Privacy Statement