De-magnetize part after surface grinding with AC tig?

Hey guys - crazy question. Trying to figure out a quicker easier way to de-magnteize some parts that I had machined. They were machined on a magnetic base table so they have become magnetized. I read that you can de-magnetize with heat (very hot, too hot for these parts), hammering (out, I need to preserve the finish on these), or AC current. The only thing I could think of that had decent AC generation was my TIG welder lol.

Could I hit my TIG welder to these steel pieces just to let it flail the arc around on the non critical surfaces to de-magnetize? Or, does it require the AC magnetic field of an AC source? Bah!

Any ideas?
__________________
Miller Diversion 180
Hobart Handler 140 (Soon to be replaced with Miller 211?)
Miller Spectrum 625 Extreme
Reply With Quote
  #2  
Old 07-06-2012, 04:07 PM
papaharley03's Avatar
papaharley03 papaharley03 is online now
WeldingWeb Craftsman
 
Join Date: Feb 2011
Location: Near Dallas, TX
Posts: 1,318
Re: De-magnetize part after surface grinding with AC tig?

Find or make a degaussing coil like the ones they used on CRT tv sets before the sets had the coil built in. Or, find a bulk magnetic tape eraser which does the same thing but was made for use on open reel tapes.

Papa
__________________
Lincoln Idealarc 250 (circa 1962)
Lincoln Weldpak 155 w/Mig Kit
Lincoln Squarewave TIG 175
Reply With Quote
  #3  
Old 07-07-2012, 08:50 AM
Bob_C Bob_C is online now
WeldingWeb Apprentice
 
Join Date: Dec 2011
Location: MA
Posts: 49
Re: De-magnetize part after surface grinding with AC tig?

Several years ago I was able to degause a large CRT monitor with a Weller soldering gun. I just turned the gun on and passed it slowly around the monitor about an inch or two from the screen for 2-3 min. It worked like a charm.

I don't know if it would work for your problem but its worth a try.

Bob
Reply With Quote
  #4  
Old 07-07-2012, 11:07 AM
killdozerd11's Avatar
killdozerd11 killdozerd11 is offline
WeldingWeb Craftsman
 
Join Date: Apr 2010
Location: The Peoples Republic of California
Posts: 1,168
Re: De-magnetize part after surface grinding with AC tig?

They have de magnetizer's usually in the shop were the do surface grinding
cause you do that right after your done grinding the part

I always hated that thing because of the 60 cycle hum it gives off ...been shocked one to many times
__________________
Backed my CATMA over your CARMA oops clusmy me

What would SATAN do ??

Miller Digital Elite
Miller Trail Blazer 302 Air Pak
Suitecase 12RC
Spectrum 625 Xtreme
Victor O/A
Evolution Rage 3 saw
Rusty old Truck
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 12:24 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.