I currently have large O/A tanks,that I rent and don't use much.I just picked up some smaller tanks(B) acetylene size.Can I adapt my larger regulators to fit the smaller tanks or should I just get smaller regulators.I'm just tired of dragging around big tanks and paying rental.Thanks.
Reply With Quote
  #2  
Old 09-16-2007, 09:48 PM
o.c.d. o.c.d. is offline
WeldingWeb Tradesman
 
Join Date: Sep 2006
Posts: 200
Re: Dumb regulator question of the day

Hi 59ih340,

Yes you can get adapters. My setup is large reg's and a B acet. tank, with a Q oxy. I think the fittings are CGA-540 to CGA-520 or 510?, I'm sorry I can't be sure as I'm not home now, in NC on a buisness trip. However, any local welding supply should be able to set you up for $10 to $20 dollars.

o.c.d.
Reply With Quote
  #3  
Old 09-16-2007, 09:49 PM
tresi's Avatar
tresi tresi is offline
WeldingWeb Artisan
 
Join Date: Oct 2006
Location: Cassville, Missouri
Posts: 2,116
Re: Dumb regulator question of the day

I believe that they do make that adaptor. Just check you local welding supply shop.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 08:29 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.