These are the projects I am looking at over the next few years:
1. turbo manifold/tubing
2. SS 1.5" T-Top frame for a boat
3. Build an Aluminum boat (3/16")

Do I want to get a spoolgun MIG setup or a AC/DC tig? I prefer the TIG but for some reason boat builders all use the MIG, I don't like the complication of a spool and all the setup inconvenience when changing metals. Not sure if I could use TIG to build a small aluminum boat?
Reply With Quote
  #2  
Old 08-01-2004, 11:11 AM
axehind axehind is offline
WeldingWeb Journeyman
 
Join Date: Jan 2004
Posts: 103
I think with the variety of materials your going to be welding that TIG would be best for you.

axehind
Reply With Quote
  #3  
Old 08-01-2004, 08:55 PM
regal regal is offline
Solderer
 
Join Date: Jul 2004
Posts: 5
do you think the TIG could be used to build a boat hull without causing distortion?
Reply With Quote
  #4  
Old 08-02-2004, 06:29 AM
BSOK BSOK is offline
WeldingWeb Journeyman
 
Join Date: Mar 2004
Location: Northern, VA
Posts: 102
You will have greater control of the heat affected area on the work piece with Tig. If you use and foot petal or hand amp control you have excellent control of how much heat you are adding to the weld area. As with a spool gun set- up, when you pull the trigger you are committed to the settings that the machine was set to. I have used both Tig and Mig on Al and prefer Tig. I produce better welds with the Tig process and it is much easier to start, stop and restart the weld. The draw back may be the amount of time it takes to run the same weld bead, the Mig process is several times faster.

A Tig machine will give you greater flexibility to weld mild steel, stainless and AL. It is just a matter of changing the tungsten and using the correct filler rod. As for Mig you will need 3 types of gas for the three metals.

Good Luck with your projects.
__________________
Brian
Lincoln Mig 215
Miller 211
Victor Torch Set
Miller Maxstar 200SD
Miller Syncrowave 250DX Tig runner
Miller Trailblazer 302 running on LP
Miller Extreme 12 VS Suitcase
Ellis 1600 Bandsaw
Miller xmt350 CC/CV
Lincoln Vantage 300
Reply With Quote
  #5  
Old 08-02-2004, 10:34 PM
HWooldridge HWooldridge is offline
WeldingWeb Journeyman
 
Join Date: Mar 2004
Location: Central Texas
Posts: 136
TIG will take longer but yield higher quality welds and have greater flexibility.
__________________
Get it hot and hit it hard...
Reply With Quote
  #6  
Old 08-02-2004, 11:57 PM
Brainfarth's Avatar
Brainfarth Brainfarth is offline
WeldingWeb Craftsman
 
Join Date: Oct 2003
Location: The armpit of Portland.
Posts: 1,247
I couldn't imagine welding an entire boat via TIG. I ran .052 aluminum mig at a job and pulled off 650 feet(all position) in 8 hours while cleaning all of my welds. I've never tried to TIG any large projects from start to finish. But I bet if you do, your last weld will look like a million bucks.
__________________
Common sense in an uncommon degree is what the world calls wisdom.
Reply With Quote
  #7  
Old 08-03-2004, 10:38 AM
Sberry Sberry is offline
WeldingWeb Foreman
 
Join Date: Jan 2004
Location: Brethren, Mi
Posts: 513
My Bud bought a boat Hull recently, its like an 18 or 20 ftr, big wide thing, very sturdy, some kind of working type of boat and it was all tig welded,, o at least it sure looked tigged. Not one zit of splatter anywhere. These guys do it all the time,,, probably get fairly fast.
__________________
www.urkafarms.com
Reply With Quote
  #8  
Old 08-06-2004, 12:43 PM
regal regal is offline
Solderer
 
Join Date: Jul 2004
Posts: 5
thanks all for the help, I am going to look for a tig
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:21 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.