#1  
Old 01-27-2011, 08:47 AM
socoj2 socoj2 is offline
WeldingWeb Foreman
 
Join Date: Aug 2009
Location: Atlanta Ga
Posts: 768
Wire size for an Extension cord

I would like to make an extension cord for my Cart to haul it outside.

30 amps max But i would like to run 75 feet?

will 10-3 SOW cable be fine or do i have to go to 8-3?
Reply With Quote
  #2  
Old 01-27-2011, 10:15 AM
goinssr goinssr is offline
WeldingWeb Tradesman
 
Join Date: Aug 2010
Location: Arkansas
Posts: 338
Re: Wire size for an Extension cord

8-3......
__________________
Stephen
Millermatic 251
Miller Syncrowave 200
Miller 30A Spoolgun
Hypertherm Powermax 30
Etc., etc., etc.............
Cancer Sucks!
Reply With Quote
  #3  
Old 01-27-2011, 11:16 AM
Broccoli1's Avatar
Broccoli1 Broccoli1 is online now
Master Welder
 
Join Date: Dec 2007
Location: Los Angeles
Posts: 4,644
Re: Wire size for an Extension cord

You can use 10/3 for your MM175

It draws 20amps at the rated output of 130amps and even if you draw more amps you Can't do it for any amount of time that would affect the Cord due to the duty cycle.

If you can get the 8/3 Cord for cheap then go ahead but it is rather pricey by the Foot.

Home Depot sells a 100' 10/3 cord with 5-15 connectors, remove those and replace with 6-50 connectors.

'bout the cheapest route

$112.00 for the 1100' cord
$17.00 for the Female 6-60 connector
Amazon Amazon

$15.00 for the male 6-50 ( you can get it at Home Depot)
__________________
Ed Conley
http://www.screamingbroccoli.net/
MM252
MM211
Passport Plus & Spool gun
TA 185
Lincoln SP135 Plus- (Gone to a good home)
Miller 125c Plasma 120v
O/A set
SO 2020 bender
Beer in the fridge
Reply With Quote
  #4  
Old 01-27-2011, 12:04 PM
socoj2 socoj2 is offline
WeldingWeb Foreman
 
Join Date: Aug 2009
Location: Atlanta Ga
Posts: 768
Re: Wire size for an Extension cord

Quote:
Originally Posted by Broccoli1 View Post
You can use 10/3 for your MM175

It draws 20amps at the rated output of 130amps and even if you draw more amps you Can't do it for any amount of time that would affect the Cord due to the duty cycle.

If you can get the 8/3 Cord for cheap then go ahead but it is rather pricey by the Foot.

Home Depot sells a 100' 10/3 cord with 5-15 connectors, remove those and replace with 6-50 connectors.

'bout the cheapest route

$112.00 for the 1100' cord
$17.00 for the Female 6-60 connector
http://www.amazon.com/Hobart-770204-.../dp/B001FOPXSE

$15.00 for the male 6-50 ( you can get it at Home Depot)
I say 30 because the ill also need it for the Tig and plasma i havent bought yet.
Ill see if i can track down some 8-3
Reply With Quote
  #5  
Old 01-27-2011, 12:07 PM
Broccoli1's Avatar
Broccoli1 Broccoli1 is online now
Master Welder
 
Join Date: Dec 2007
Location: Los Angeles
Posts: 4,644
Re: Wire size for an Extension cord

probably better off just purchasing a 50' and a 25' Welder extension cord

probably gonna cost about $200.00
__________________
Ed Conley
http://www.screamingbroccoli.net/
MM252
MM211
Passport Plus & Spool gun
TA 185
Lincoln SP135 Plus- (Gone to a good home)
Miller 125c Plasma 120v
O/A set
SO 2020 bender
Beer in the fridge
Reply With Quote
  #6  
Old 01-27-2011, 01:11 PM
goinssr goinssr is offline
WeldingWeb Tradesman
 
Join Date: Aug 2010
Location: Arkansas
Posts: 338
Re: Wire size for an Extension cord

Try Ebay. I bought a very nice 50' 8-3 cord with plugs for just a bit over $100. Not a cheapy cord either.
__________________
Stephen
Millermatic 251
Miller Syncrowave 200
Miller 30A Spoolgun
Hypertherm Powermax 30
Etc., etc., etc.............
Cancer Sucks!
Reply With Quote
  #7  
Old 02-14-2011, 09:22 AM
tilelayher tilelayher is offline
WeldingWeb Apprentice
 
Join Date: Jan 2011
Location: Outisde Philly
Posts: 21
Re: Wire size for an Extension cord

not trying to thread jack, is this for a 110 machine? I need to do the same thing for my welder and I am unsure of what size cord to use. I was thinking of making my own and buying the materials from an electrical supply house,
__________________
Millermatic 130XP
Tilesetter by Trade
Reply With Quote
  #8  
Old 02-14-2011, 10:36 AM
Broccoli1's Avatar
Broccoli1 Broccoli1 is online now
Master Welder
 
Join Date: Dec 2007
Location: Los Angeles
Posts: 4,644
Re: Wire size for an Extension cord

Quote:
Originally Posted by tilelayher View Post
not trying to thread jack, is this for a 110 machine? I need to do the same thing for my welder and I am unsure of what size cord to use. I was thinking of making my own and buying the materials from an electrical supply house,
For a 120v machine 100'

HD sells a Ridgid 10/3 Cord with the correct 120v ends on it

but I would buy 2 12/3 50' cords
__________________
Ed Conley
http://www.screamingbroccoli.net/
MM252
MM211
Passport Plus & Spool gun
TA 185
Lincoln SP135 Plus- (Gone to a good home)
Miller 125c Plasma 120v
O/A set
SO 2020 bender
Beer in the fridge
Reply With Quote
  #9  
Old 02-15-2011, 01:21 PM
Mundy's Avatar
Mundy Mundy is offline
WeldingWeb Apprentice
 
Join Date: Mar 2008
Location: Michigan
Posts: 12
Re: Wire size for an Extension cord

I notice a huge diffence in how my 120 volt welder runs when plugged into a 25' 12-3 cord compaired to my new 50' 10-3 cord.
Both cords were plugged into the same outlet.

One morning I had welded up some brackets with the welder plugged into it ussual outlet in the barn. It ran great as ussual. Then I needed to weld the brackets to the trailer but needed an extention cord to reach. so I grabbed my shortest big cord I had, a 25' 12-3 cord. I laid down a couple welds fighting it the whole way and ended up grinding them all out.
I took the welder back into the barn thinking something was wrong with it. I plugged it into the outlet and it was back to welding good like before. I called my electrician buddy and he brought over a 10-3 50' cord put ends on it and my welder runs just like its plugged into the wall.

I am not sure about braided verses solid but I know the wireing to the plug in the barn is 12-3 solid and the cords are braided. I think that is the differnce?
__________________
Regards,
Mundy
Reply With Quote
  #10  
Old 02-15-2011, 02:36 PM
tilelayher tilelayher is offline
WeldingWeb Apprentice
 
Join Date: Jan 2011
Location: Outisde Philly
Posts: 21
Re: Wire size for an Extension cord

I got as 100 ft 10/3 cord this thing is thick I shall see what it does when plugged in.
__________________
Millermatic 130XP
Tilesetter by Trade
Reply With Quote
  #11  
Old 02-15-2011, 05:19 PM
nadogail nadogail is offline
WeldingWeb Foreman
 
Join Date: Jan 2011
Location: Coronado. CA across the bay from San Diego, CA
Posts: 630
Re: Wire size for an Extension cord

Braided, we call it stranded, versus Thick, we call it stranded.

There is no difference in the electrical conductivity between these two kinds of wire, at 60 HZ.

Stranded is generally preferred because it is more flexible and resists damage from vibration. Solid is less expensive, and easier to connect to receptacles (outlets).

Most buildings are built to meet a price, not a quality.
__________________
I offer three choices: Good, Fast, & Cheap. You may pick two.

Hobart AC/DC StikMate LX
Harbor Freight AD Hood
Harbor Freight Industrial Chop Saw
DeVilbis 20 Gallon, 5 HP Compressor
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:03 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.