#1  
Old 06-27-2011, 09:32 PM
Oatsy's Avatar
Oatsy Oatsy is offline
WeldingWeb Journeyman
 
Join Date: May 2010
Location: North Carolina/Vermont
Posts: 93
MIG aluminum. What ya think?

First off I'll start by saying this is the first time I have ever welded aluminum with my machine. Prior to today I have only practiced aluminum once and the machine was already set up for me, I ran a few beads just to try it and that was it. I have wanted to learn to weld aluminum for quite some time now and finally gave it a go tonight. Heres a few pictures after about an hour or so of experimenting with different settings and travel speed.




Certainly not the prettiest welds but I am very happy with how they turned out
Setup:
Clarke 180EN no spool gun. (i heard after they went out of business here the machines are made in china? luckily mines an old one.)
ER5356 .030 wire
100%argon at about 6-7 cf/h
base metal was 16 gauge i believe.
Full penetration
Any suggestions on things I should make changes to? I have a few projects I want to do soon but I will continue to practice a bit more before I jump into anything too serious. And yes I know about how to avoid the burn through at the end of my weld, this was just me practicing my bead.
__________________
Reply With Quote
  #2  
Old 06-28-2011, 12:58 PM
shovelon's Avatar
shovelon shovelon is offline
WeldingWeb Artisan
 
Join Date: Dec 2010
Location: SoCal-LA
Posts: 2,965
Re: MIG aluminum. What ya think?

Ya need more gas bro.

For a 1/2" orafic nozzle, you need at least 20cfh.
Reply With Quote
  #3  
Old 06-28-2011, 04:37 PM
Oatsy's Avatar
Oatsy Oatsy is offline
WeldingWeb Journeyman
 
Join Date: May 2010
Location: North Carolina/Vermont
Posts: 93
Re: MIG aluminum. What ya think?

I'll try turning it up to 20 or a little more. I had turned it up to around 17cfh while i was still experimenting and the results appeared to be the same as with running lower cfh. With more practice I think I can lay down some nicer looking beads, maybe even as nice as my steel beads.
__________________
Reply With Quote
  #4  
Old 06-30-2011, 01:06 PM
shovelon's Avatar
shovelon shovelon is offline
WeldingWeb Artisan
 
Join Date: Dec 2010
Location: SoCal-LA
Posts: 2,965
Re: MIG aluminum. What ya think?

Are you pushing the bead? That is the recommended direction for mig alum.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 02:51 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.