can ya fix me tractor bit
had a bloke come in to day need a manifold for is tractor patch up till he can find another one
it was in a sad way bits disappeared when I was grinding it so I had alot of building up to do in the end it turned out ok the build up weld isn't the pretty but didn't need to seen it was getting sanded to shape this should keep him going before inbetween after lots of build done
__________________
Creative metal A married man should forget his mistakes. There's no use in two people remembering the same thing! |
|
#2
|
|||
|
|||
|
Re: can ya fix me tractor bit
now just repaint it and it will look new, good job
__________________
![]() Chuck ASME Pressure Vessel welder |
|
#3
|
||||
|
||||
|
Re: can ya fix me tractor bit
Quite the job!
David
__________________
Real world weldin. ![]() When I grow up I want to be a tig weldor.
|
|
#4
|
|||
|
|||
|
Re: can ya fix me tractor bit
very nice!
__________________
Idealarc 300\300 TIG AC\DC |
|
#5
|
||||
|
||||
|
Re: can ya fix me tractor bit
now i bet he stops looking for a new one, after all with a fix like that he will likely bring you the other side.LOL
thats a lot of build up for TIG, was it TIG ?? the one on the right looks like tig but hard to tell on the big one up front.
__________________
summer is here, plant a tree for mother earth. if you dont have time or space, sponcer some one else to plant one for you. ![]() feel free to shoot me a PM or e-mail me at [email]james@newyorkmetalart.com i got lots of time.
|
|
#6
|
||||
|
||||
|
Re: can ya fix me tractor bit
yeah it was done with the tig fun4now took about 2 1/2 hours to do all 3 outlets and weld the fitting on
__________________
Creative metal A married man should forget his mistakes. There's no use in two people remembering the same thing! |
|
#7
|
||||
|
||||
|
Re: can ya fix me tractor bit
Good job.... Hope he appreciates your efforts. did you have to re-shape the exhaust ports as well?
__________________
_________________ Chris
|
|
#8
|
||||
|
||||
|
Re: can ya fix me tractor bit
Quote:
David
__________________
Real world weldin. ![]() When I grow up I want to be a tig weldor.
|
|
#9
|
||||
|
||||
|
Re: can ya fix me tractor bit
Quote:
__________________
Creative metal A married man should forget his mistakes. There's no use in two people remembering the same thing! |
|
#10
|
||||
|
||||
|
Re: can ya fix me tractor bit
Quote:
__________________
_________________ Chris
|
|
#11
|
|||
|
|||
|
Re: can ya fix me tractor bit
wello, did those just corrode to peices like that? wow.
__________________
Various Grinders Victor Journeyman torch 200cf Acet. 250cf oxygen Lincoln 175 plus/alpha2 gun Lincoln v205t tig Lincoln 350mp Esab 650 plasma When you can get up in the morning, Its a good day. Live each day like its your last. |
|
#12
|
||||
|
||||
|
Re: can ya fix me tractor bit
Nice job Wello.
- Paul
__________________
Hold my beer...watch this. |
![]() |
| Thread Tools | |
| Display Modes | |
|
|