I have heard wonderful and at times remarkable stories and reports from guys using Certanium rods.
These are expensive rods! Why?

When I went to the local welding supplier, and spoke to him about rods to use to weld disimilar metals, among the many we spoke about, I mentioned Certanium rods, and he said Certanium does not manufacture there own rods, they buy others rods and remark and re package them, and sell at exorberant prices. You can buy the same rod from the original manufacturer cheeper.

So I want to know , is what the local store rep. says about Certanium, true?

If so, then who, or what manufactuer do I contact to get the same rod from, only cheeper?
Flywelder
3-06-07
Reply With Quote
  #2  
Old 03-08-2007, 12:08 AM
ss42768 ss42768 is offline
WeldingWeb Tradesman
 
Join Date: Apr 2006
Posts: 225
Re: Questions about Certanium rods

I run across these rods once in a while, and yes they are extremely high priced. The local store rep should be able to cross this rod over for you, either to a JW Harris Welco product or check out Esab, they have a lot of maintenance alloys as well. I've quoted against this company several times and have always come out on top, the biggest problem I have is that customers think since my rod is so much cheaper that it must not be as good. I'm not sure but I think Certanium might be tied in with Rockmount Alloys.
Reply With Quote
  #3  
Old 03-10-2007, 02:08 AM
Flywelder Flywelder is offline
WeldingWeb Apprentice
 
Join Date: May 2006
Location: NC
Posts: 19
Thumbs up Re: Questions about Certanium rods

Thanks for this info!
I'll look into them right away!
Flywelder
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 12:05 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.