| Register | FAQ | Members List | Calendar | Search | Today's Posts | Mark Forums Read |
![]() |
|
|
Thread Tools | Display Modes |
|
#51
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
So, how does one order a 250EXT? What is the pricing? Thanks, Geoff.
|
|
#52
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Geoff,
We are out of stock again, but will have some more soon.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#53
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
What is the pricing and what is "soon"? Is the warranty five years, or does it fall under the new three year warranty policy? Thanks, Geoff.
|
|
#54
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
I expect early-mid Feb. As we announced all AC/DC tigs will all under the 3+2 year program.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#55
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Why the warranty change? When I looked at your site it still said five year warranty ... is the +2 a extended plan. ? If so what's the pricing?
|
|
#56
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
any one taying a pention?
|
|
#57
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Quote:
will take us few month to get all done correctly
__________________
Oleg Gadshteyn oleg@everlastwelders.com www.everlastgenerators.com/ 650 588 8588 x201 www.linkedin.com/pub/oleg-gladshteyn/48/b08/875 |
|
#58
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Agreed!! Shame
__________________
Thermal Arc Fabricator 210 1970 Lincoln Redface Miller 150 STL Still need a Syncrowave and a plasma and a milling machine and a lathe and a bigger shop and a.... My other addictive hobby; http://frozenpixels.smugmug.com/ |
|
#59
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
well heres the deal, i plan on buying one in the next couple of weeks. so i would like to know what the deal is before i hand over my money........ It seems the only one you can get a straight answer from is lug........
|
|
#60
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
The knobs are still available on the EX. You can't have digital control with memory without buttons.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#61
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Until we get the new warranty posted the current one is still in effect.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#62
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
thank you for the clear response Lug.
|
|
#63
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
How does the 250ext machine work with anodized aluminum? Has any testing been done?
|
|
#64
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
With the amplitude offset, (ability to set half cycle AC + and - amps relative to each other) it works quite well.The cleaning lines can virtually disappear, while maintaining a good puddle.
__________________
Welders: Esab Migmaster 250 Penncraft 230 (oldy but goody) HF Plasma 30 (Italian) Lincoln Ranger 8 Smith Oxy/Acetylene/Propane Lincoln SA200 Everlast Power Tig 250 EX Everlast PowerUltra 205 |
|
#65
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Quote:
Ive Looked a lot at Longevety on You Tube,and talked to alot of there "stars" on U tube,,I was after Ron for so Long to get a 250 tig,,and they would FLY off the shelf,But under his Problems,I understand why,he had more pressing thing on his mind,, So,how can you sell me on selling Everlast???? over Longevety?? As I really like what they have to offer,and being in the welding business for 35+ years,I just didnt fall of the turnip truck,,Just seems here,and Believe me,I did not come here to start trouble,But,seems theres no leader?????? Thanks,Jack Connors! ![]() PS,, Longevety DOES NOT KNOW!!!!!!,Im even posting this,,,FYI!!!!!!!,,Thanks again,Jack Last edited by Storts; 03-25-2012 at 02:15 AM. Reason: Add |
|
#66
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Hello Jack
please email me your number and i will cal you will tell you all about the warranty and difference between Everlast the other other company
__________________
Oleg Gadshteyn oleg@everlastwelders.com www.everlastgenerators.com/ 650 588 8588 x201 www.linkedin.com/pub/oleg-gladshteyn/48/b08/875 |
|
#67
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Let me test out your AC machine...We can give it a workout and test it.....
WWW.CMGANGWAYS.COM WWW.TRAILERWORX.COM ![]() ![]() ![]()
|
|
#68
|
||||
|
||||
|
Boney
Call and order one.. Then you can report back Oleg Gladshteyn Oleg@everlastwelders.com 415 613 664 cell 650 588 8588 work
__________________
Oleg Gadshteyn oleg@everlastwelders.com www.everlastgenerators.com/ 650 588 8588 x201 www.linkedin.com/pub/oleg-gladshteyn/48/b08/875 |
|
#69
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
LOL....I would kill that thing in a week....
lol.....great machine for the GUY WHO DOES SMALL HOMEOWNER JOBS..Figured I would put it thru a few big gangways and see if it could hold up to the task that the miller dynasty or syncrowave...
|
|
#70
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Well, buy it and i will give you 6 month money back . if you kill i will refund 100% and cover shipping back
__________________
Oleg Gadshteyn oleg@everlastwelders.com www.everlastgenerators.com/ 650 588 8588 x201 www.linkedin.com/pub/oleg-gladshteyn/48/b08/875 |
|
#71
|
|||
|
|||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Quote:
Can't beat that!!! |
|
#72
|
||||
|
||||
|
Re: 2011 Everlast PowerTig 250EXT & 315EXT Tig/Stick PULSE DIGITAL WELDER
Did you order one? from the guy that parks a small forklift on a piece of aluminum gang plank and claims it supports 11,000 lbs, you do know most of the weight on an unloaded fork lift is on the rear wheels and that you have to divide the weight by 4 as you have 4 wheels.
__________________
Airco 330A/BP. Lincoln SP250 W/ spoolgun, GoWeld x2 TA Predator, ESAB 300AVS Feeder ESAB 875 plasma. . Bernard Cooler. Evo 355. OA Demo: Longevity Tigweld 200SX, Forcecut 42i Everlast 140ST.. On loan to friend/sale pending |
![]() |