CNC Plasma Table

This is our 3rd table to build. It is built very sturdy and performs very well. It utilizes many things found on high end system costing over 15K. We built this table to sell, it has a couple of hours of use on it.

Pictures & Videos: https://picasaweb.google.com/1053800...79/April232012

Our website: NorthridgeFab.com

Email: NorthridgeFab (at) gmail (dot) com

Phone: 970.626.sixty ninety

Spec's:

Cut Area: 48x60

Table Size: 55x65

Gantry Parking area

30mm linear bearing slide on X & Y axises

15mm linear bearing slides on Z axis

Advanced Height Control w/Floating Head

Tall clearance gantry for cutting SQ tubing, Channel, I-Beams, Etc.

Dual side drive gantry

6" deep water table.

Curved slats

Rack & Pinion drives

3:1 reduction on X & Y axises via timing belts/pulleys

5 Start Z axis acme screw

All motors are Hybrid 620oz steppers w/Gecko Drives

CandCNC Controls w/custom Mach3 Screens

Dell Desktop

SheetCAM

Mach3 (Already calibrated to table)

The plasma cutter and torch are not included in the price. If your interested in them, contact us.

We are located in western Colorado. Pickup is welcome or we can deliver the machine any where in the US for 1.25-1.65 per loaded mile depending on distance.

8950.00 obo
__________________
Northridge Fabrications
Montrose, CO
970.626.6090

NorthridgeFabrications.com
Reply With Quote
  #2  
Old 05-27-2012, 09:23 PM
Sparky0908 Sparky0908 is offline
WeldingWeb Journeyman
 
Join Date: Jan 2011
Location: St. Louis
Posts: 119
Re: CNC Plasma Table

Do you have pics?
Reply With Quote
  #3  
Old 05-27-2012, 10:50 PM
Ron Padilla Ron Padilla is offline
WeldingWeb Foreman
 
Join Date: May 2010
Location: use to be Lake Elsinore, Ca now Clarksville Tn
Posts: 620
Re: CNC Plasma Table

there is a link in the post above for photos
Reply With Quote
  #4  
Old 05-27-2012, 10:56 PM
MoroneysWelding MoroneysWelding is offline
WeldingWeb Journeyman
 
Join Date: Sep 2008
Location: South Florida
Posts: 73
Re: CNC Plasma Table

Love it man. Only concern is that it seems the water and sparks are landing on the electronics under the table.
__________________
Millermatic 251
Miller Bobcat 225
Lincoln 135
Victor Oxy/Fuel
Older Thermal Dynamics 50 amp (paid $700 with 10 sets of consumables)
Reply With Quote
  #5  
Old 05-28-2012, 07:57 AM
BryanDowdy's Avatar
BryanDowdy BryanDowdy is offline
WeldingWeb Journeyman
 
Join Date: Oct 2005
Location: Montrose, CO
Posts: 116
Re: CNC Plasma Table

Quote:
Originally Posted by MoroneysWelding View Post
Love it man. Only concern is that it seems the water and sparks are landing on the electronics under the table.
Thanks. The top of the enclosure has gotten a few drops, but nothing inside. I will look at moving it inward.
__________________
Northridge Fabrications
Montrose, CO
970.626.6090

NorthridgeFabrications.com

Last edited by BryanDowdy; 05-28-2012 at 08:15 AM.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:02 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.