Looking at getting another regulator for back purging

What are your thoughts on getting a 2nd regulator and using my "old" 80 cubic argon bottle vs getting a dual output single regulator for my 330 (i think) cubic argon bottle?

My 330 is near my welder which isn't totally near where I work, so the 80 could be nmoved and be a dedicated purging/back up bottle.

If getting a 2nd regulator for a 2nd bottle, which is where I am leaning, is there any benefit to just getting a 2nd identical regulator (I have the one that came with my Diversion, a smith dial type) or does a flowmeter style one offer much benefit? I've got friends who weld and use flowmeter type, but I don't know if it matters much:



Looking at the Smith 30 series flowmeter

Thanks guys
__________________
Miller Diversion 180
Hobart Handler 140 (Soon to be replaced with Miller 211?)
Miller Spectrum 625 Extreme
Reply With Quote
  #2  
Old 05-25-2012, 05:09 PM
farmall farmall is offline
Master Welder
 
Join Date: Aug 2009
Posts: 3,911
Re: Looking at getting another regulator for back purging

Getting two separate regs has one VERY nice benefit.

If you break part of a double regulator, you lose the whole thing for a while.

If you have two regs on an Western CGA-580 manifold tee (about 27 bucks), you take them both off the tee and put the good one on your cylinder.

You can use the regs on separate cylinders or together on one cylinder.

Tees are cheap (about 28 bucks) they work great, and have no downside.

Search for:

Western Enterprises 312-T-92: Manifold Coupler Tees
Reply With Quote
  #3  
Old 05-25-2012, 07:51 PM
snoeproe snoeproe is offline
WeldingWeb Craftsman
 
Join Date: Apr 2008
Location: NW ON Canada
Posts: 1,060
Re: Looking at getting another regulator for back purging

I use that same Smith regulator/flowmeter on my tig. It has been good.
__________________
Jason
Lincoln Idealarc 250 stick/tig
Thermal Dynamics Cutmaster 52
Torchmate CNC table
I.A.M. Local 771

Owner/Operator Devlin Metal Works
Custom CNC Plasma Cutting and Welding
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:36 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.