cutting stainless for exhaust

I'm curious what everyone here would suggest for cutting 304 stainless 16g 3" tubing. I've got a tiny 1.5 car garage that doesn't have much room for a. Stationary bandsaw, so I've been eyeballing an Evolution 14" Rage 2. Chop saw for the occasional stainless exhaust work on my friends cars or my truck and turbo build. The main use will be for chopping exhaust tube and maybe some mild sch 40 peices for a turbo maifold.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #2  
Old 07-03-2012, 02:10 AM
rabidchimp rabidchimp is offline
WeldingWeb Foreman
 
Join Date: May 2012
Location: Lakewood, WA
Posts: 572
Re: cutting stainless for exhaust

I've heard those saws don't do too well on the stainless, but I've cut plenty of similarly sized material on a regular chop saw, $179 will get you a nice Ridgid 14" saw.
-Aaron
__________________
Hardinge HC Chucker Lathe --- Jet 17.5" Drill Press
Lincoln 175 MIG, 175 Square Wave TIG, Power Mig 256
Dewalt 14" Chop Saw - Victor O/A Setup
Jet 7x12 Horizontal ---- Jet 17" Vertical
https://www.facebook.com/#!/RabidChimpPerformance
Reply With Quote
  #3  
Old 07-03-2012, 02:58 AM
DougAustinTX's Avatar
DougAustinTX DougAustinTX is offline
WeldingWeb Tradesman
 
Join Date: Oct 2009
Location: Austin TX
Posts: 444
Re: cutting stainless for exhaust

Agreed on the chop saw. I just finished a 4" stainless dual exhaust on a '69 Camaro and all cuts were made on the chop saw. Then outside edges were trued and deburred on a stationary belt sander, while inside edges were deburred with a carbide burr. I mig a few spot welds in place while under the car to get the angles right, then remove to tig.
__________________
Miller Syncrowave 350
Millermatic 252/ 30A spoolgun
Miller Bobcat 225g w/ 3545 spoolgun
Lincoln PowerArc4000
Lincoln 175 Mig
Lincoln 135 Mig
Everlast 250EX Tig
Century ac/dc 230 amp stick
Victor O/A
Hypertherm 1000 plasma
Reply With Quote
  #4  
Old 07-03-2012, 10:38 AM
Albie Albie is offline
WeldingWeb Journeyman
 
Join Date: Feb 2012
Location: NE Penna.
Posts: 72
Re: cutting stainless for exhaust

Got a Rage 2 last year. Cuts square tube 2"x1/4 and same same angle great. Still using the supplied blade, which is kind of a universal. Have to get a better blade for steel and a blade for stainless. Needs a dedicated blade for certain materials. To me, it is way better than a abrasive type saw. Opinions will differ.
Reply With Quote
  #5  
Old 07-03-2012, 12:18 PM
Donoharm's Avatar
Donoharm Donoharm is online now
WeldingWeb Tradesman
 
Join Date: Oct 2010
Location: The Netherlands
Posts: 370
Re: cutting stainless for exhaust

angle grinder + cutting disc 1mm + wraparound
__________________
--------------------------------------------------------------
www.inoxworks.eu
Reply With Quote
  #6  
Old 07-03-2012, 12:36 PM
fortyonethirty fortyonethirty is offline
WeldingWeb Foreman
 
Join Date: May 2009
Location: San Luis Obispo, CA
Posts: 758
Re: cutting stainless for exhaust

Abrasive is the way to cut thin stainless. Stainless will dull the carbide blades very quickly. And on the thin stuff the carbide blades tend to "grab" the material and deform it or fling it across the shop.

A disc sander works well for squaring the cut ends, belt sander also works well, but I prefer the disc.
__________________
Ian Tanner

Kawasaki KX450f and many other fine tools
Reply With Quote
  #7  
Old 07-03-2012, 01:58 PM
Jürgen's Avatar
Jürgen Jürgen is offline
WeldingWeb Journeyman
 
Join Date: Jun 2012
Location: Bellevue, WA
Posts: 66
Re: cutting stainless for exhaust

I have a Makita LC1230 dry cut saw with a blade for stainless. The blade is about $200.
Not a cheap solution, but the cuts are perfect with no sparks.
Reply With Quote
  #8  
Old 07-03-2012, 07:07 PM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

I've read some reviews on the Evolutions chop and you can get them for 309 shipped online with a multi metal blade. Some of the automotive fab guys on Honda-tech use them in their shops and have nothing but positive things to say about them. I've also been keeping an eye on craigslist for a used ridged or Millwakee chop saw and just picking up a 14" blade for stainless. I've used chop saws at work for cutting metal studs and they worked fine, I just disliked changing the abrasive blades.

I've built a 2.5 to 3" stainless y pipe and full exhaust for the stainless headers on my 95 Dakota sport using just a cut off wheel and a hacksaw and it sucks. Then I still need to fab a downpipe for my turbo ecotec project and my buddy's turbo cavalier build as well and I'm not going to spend forever hacking away and swapping blades every 2-5 cuts.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #9  
Old 07-06-2012, 11:49 PM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

Well I just picked up a milwakee porta band deep cut for 150 so this will hold me over till I get a chop saw.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #10  
Old 07-07-2012, 10:45 AM
VPT's Avatar
VPT VPT is offline
WeldingWeb Craftsman
 
Join Date: Dec 2009
Location: Stevens Point, WI
Posts: 1,296
Re: cutting stainless for exhaust

I was just going to post to look for a portable band saw. They aren't as versatile as say a sawzal but they do a great job!
Reply With Quote
  #11  
Old 07-07-2012, 11:00 AM
Showdog75 Showdog75 is offline
WeldingWeb Foreman
 
Join Date: Mar 2010
Location: East Tennessee
Posts: 652
Re: cutting stainless for exhaust

Quote:
Originally Posted by pushrods View Post
Well I just picked up a milwakee porta band deep cut for 150 so this will hold me over till I get a chop saw.
Now buy yourself the fixture that swag offroad sells for a port a band and you will have yourself a nice set-up.
Reply With Quote
  #12  
Old 07-07-2012, 07:47 PM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

Thanks for the input on the fixture I'll look into that.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #13  
Old 07-07-2012, 10:17 PM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

Showdog- that is one cool add on for the portaband......I'm going to order one shortly. Thanks again for the tip.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #14  
Old 07-07-2012, 11:01 PM
walker walker is offline
WeldingWeb Foreman
 
Join Date: Sep 2005
Location: Cave Creek AZ
Posts: 657
Re: cutting stainless for exhaust

I bought one of the Evolution hand held metal cutting saws. I won't buy another Evolution product. I also agree with either the zip wheels or abrasive for what you are doing.
Reply With Quote
  #15  
Old 07-12-2012, 12:02 AM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

Thanks fo the input guys, I'll use my 4 /2 cutoff wheels and my porablt milwakee band saw. I just placed an order for v3.0 poraband table and can't wait for it to arrive.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #16  
Old 07-12-2012, 07:09 AM
OffshoreNDT OffshoreNDT is offline
WeldingWeb Apprentice
 
Join Date: Mar 2008
Posts: 32
Re: cutting stainless for exhaust

thanks for the recomendation to swag offroad awesome stuff on there
Reply With Quote
  #17  
Old 07-17-2012, 10:13 AM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

Just n update, my swag offroad v3.0 table came in on Saturday and it kicks some ***. I love how easy this simple add on made things for me in the garage. I took some 16g 3" 304 stainless tube and made a tight radius 90degree bend for my turbo cavalier build after work tonight. Went very well andhere are some pics.



__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
  #18  
Old 07-17-2012, 12:53 PM
rabidchimp rabidchimp is offline
WeldingWeb Foreman
 
Join Date: May 2012
Location: Lakewood, WA
Posts: 572
Re: cutting stainless for exhaust

Nice work there. I never liked cutting tube on a vertical band saw. I need to get a metal cutting blade for my vertical Jet. Its a big bastard I got for super cheap when a local wrecking yard went outta business. They used it for cutting down radiators.
-Aaron
__________________
Hardinge HC Chucker Lathe --- Jet 17.5" Drill Press
Lincoln 175 MIG, 175 Square Wave TIG, Power Mig 256
Dewalt 14" Chop Saw - Victor O/A Setup
Jet 7x12 Horizontal ---- Jet 17" Vertical
https://www.facebook.com/#!/RabidChimpPerformance
Reply With Quote
  #19  
Old 07-19-2012, 09:43 PM
VPT's Avatar
VPT VPT is offline
WeldingWeb Craftsman
 
Join Date: Dec 2009
Location: Stevens Point, WI
Posts: 1,296
Re: cutting stainless for exhaust

Sorry for the small pic but there is also this attachment for the band saw essentially turning it into a horizontal band saw. Also a very nice deal and great for a small shop. Helps 100% to make pipe cuts like you want to do.


Last edited by VPT; 07-19-2012 at 09:47 PM.
Reply With Quote
  #20  
Old 07-19-2012, 09:44 PM
VPT's Avatar
VPT VPT is offline
WeldingWeb Craftsman
 
Join Date: Dec 2009
Location: Stevens Point, WI
Posts: 1,296
Re: cutting stainless for exhaust

In fact now that you have the tools you could probably make that attachment.
Reply With Quote
  #21  
Old 07-23-2012, 01:44 AM
pushrods pushrods is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Location: Chicagoland
Posts: 20
Re: cutting stainless for exhaust

VPT I did see that pic and actually the bandsaw case has a small booklet with parts and whatnot and that is listed in there but way to pricey for me. The Swag table fits the bill perfectly for now.
__________________
Hobart Handler 187,
Craftsman drill press,
Smith torch setup,
Htp invertig221,
Milwakee portaband saw w/Swagoffroad V3.0 table kit
Reply With Quote
Reply

Tags
chop saw, evolution, rage2

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


All times are GMT -4. The time now is 04:51 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.