#1  
Old 07-23-2012, 11:57 AM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Bbq/smoker question

Good morning.. I am building a offset fire box style smoker out of a 120 gallon water well tank. The outside of the tank looks to be painted. But the inside has some kind of smooth coating in it. Almost like the inside of an oven or washing machine. Can anyone tell me what that coating may be? Is it safe to cook with? I tried sandblasting it and it takes a lot to get this stuff off. Even tried a torch to burn it off and it didnt phase it. Any help would be great
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #2  
Old 07-23-2012, 12:10 PM
yakdung yakdung is offline
WeldingWeb Foreman
 
Join Date: Nov 2011
Posts: 512
Re: Bbq/smoker question

Epoxy/Phenolic liner possibly? Common in food grade 55 gallon drums. Would the color of the liner possibly be red by any chance?
http://www.google.com/imgres?q=epoxy...r:12,s:9,i:144

Last edited by yakdung; 07-23-2012 at 12:13 PM.
Reply With Quote
  #3  
Old 07-23-2012, 12:24 PM
ThorsHammer's Avatar
ThorsHammer ThorsHammer is offline
WeldingWeb Artisan
 
Join Date: Jul 2011
Location: Western Washington
Posts: 2,099
Re: Bbq/smoker question

Could also be a ceramic liner that's cooked on.
__________________
There are no problems. There are only solutions. It's your duty to determine the right one.

Hobart Handler 210
Airco 225 Amp MSM Stinger
Reply With Quote
  #4  
Old 07-23-2012, 12:51 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

Quote:
Originally Posted by yakdung View Post
Epoxy/Phenolic liner possibly? Common in food grade 55 gallon drums. Would the color of the liner possibly be red by any chance?
http://www.google.com/imgres?q=epoxy...r:12,s:9,i:144
No its a deep blue color. My buddy thinks its some kind of ceramic coating. Just trying to get more input.
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #5  
Old 07-23-2012, 12:56 PM
ThorsHammer's Avatar
ThorsHammer ThorsHammer is offline
WeldingWeb Artisan
 
Join Date: Jul 2011
Location: Western Washington
Posts: 2,099
Re: Bbq/smoker question

If it's that hard to get off, and you've had a VERY hot fire in it, you'll be fine. because you're going to be cooking at far lower temps.
__________________
There are no problems. There are only solutions. It's your duty to determine the right one.

Hobart Handler 210
Airco 225 Amp MSM Stinger
Reply With Quote
  #6  
Old 07-23-2012, 01:04 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

Ok have not had any fires in it yet. I just cut the fire box off one side of the tank and thought the tank looked in to good of shape inside for being 40 yrs old. Then i found this coating. Now Ive put a hold on tjis project until I know for sure
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #7  
Old 07-23-2012, 01:39 PM
weldbead weldbead is offline
WeldingWeb Artisan
 
Join Date: Jan 2008
Posts: 3,308
Re: Bbq/smoker question

heat up a spot with a rosebud and whack it with a tenpound hammer..see how it looks aftert that and decide if you wanna eat out of it..
Reply With Quote
  #8  
Old 07-23-2012, 02:12 PM
DanD78 DanD78 is offline
WeldingWeb Tradesman
 
Join Date: Feb 2009
Location: Central Illinois
Posts: 215
Re: Bbq/smoker question

If it is a glass lined tank I would not use it for food safety reasons. I agree, hit it with a hammer and see what happens.

Dan
Reply With Quote
  #9  
Old 07-23-2012, 02:16 PM
Scott0303's Avatar
Scott0303 Scott0303 is offline
WeldingWeb Apprentice
 
Join Date: May 2012
Location: Winston Salem, NC
Posts: 23
Re: Bbq/smoker question

Does the tank have a name plate on it?
Reply With Quote
  #10  
Old 07-23-2012, 02:28 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

Quote:
Originally Posted by Scott0303 View Post
Does the tank have a name plate on it?
Yes sir it does.
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #11  
Old 07-23-2012, 02:43 PM
Scott0303's Avatar
Scott0303 Scott0303 is offline
WeldingWeb Apprentice
 
Join Date: May 2012
Location: Winston Salem, NC
Posts: 23
Re: Bbq/smoker question

Name? Company still in business? If they are still in business then they probably know what kind of liner is in it.
Reply With Quote
  #12  
Old 07-23-2012, 02:50 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

If this tank does not work out, what would be a good base to start with? I would like something at least 24" in diameter like the peice i have now.
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #13  
Old 07-23-2012, 03:10 PM
yakdung yakdung is offline
WeldingWeb Foreman
 
Join Date: Nov 2011
Posts: 512
Re: Bbq/smoker question

Quote:
Originally Posted by Jwgrillin View Post
If this tank does not work out, what would be a good base to start with? I would like something at least 24" in diameter like the peice i have now.
Build a UDS utilizing an unlined 55 gallon drum. An offset pit requires a lot of babysitting to keep the fire stoked. I can get 16 - 24 hours burn at 225 degrees without adding fuel. Check out the mother of all threads on the UDS:
http://www.bbq-brethren.com/forum/sh...ad.php?t=23436

Last edited by yakdung; 07-23-2012 at 03:12 PM.
Reply With Quote
  #14  
Old 07-23-2012, 03:15 PM
yakdung yakdung is offline
WeldingWeb Foreman
 
Join Date: Nov 2011
Posts: 512
Re: Bbq/smoker question

Care to tell us?
Reply With Quote
  #15  
Old 07-23-2012, 03:22 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

Thats the hole fun in smoking drinkin beer while you babysit the firebox
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #16  
Old 07-23-2012, 03:28 PM
yakdung yakdung is offline
WeldingWeb Foreman
 
Join Date: Nov 2011
Posts: 512
Re: Bbq/smoker question

Quote:
Originally Posted by Jwgrillin View Post
Thats the hole fun in smoking drinkin beer while you babysit the firebox
Approximately cook time for a 12 - 15 pound brisket is one hour plus per pound. I have better things to do with my time.
Reply With Quote
  #17  
Old 07-23-2012, 07:01 PM
Meat man Meat man is offline
WeldingWeb Apprentice
 
Join Date: Feb 2009
Location: Wamego, KS
Posts: 34
Re: Bbq/smoker question

It is a ceramic liner. Almost impossible to completely remove.

I suggest you find a different tank.
Reply With Quote
  #18  
Old 07-23-2012, 07:35 PM
ThorsHammer's Avatar
ThorsHammer ThorsHammer is offline
WeldingWeb Artisan
 
Join Date: Jul 2011
Location: Western Washington
Posts: 2,099
Re: Bbq/smoker question

Why not use it if it's ceramic? your house hold oven is ceramic lined. It's cooking at higher temps just fine. so you would have nothing to worry about with your offset. the ceramic is going to be harder, and last longer than anything else that could be put in it. not to mention it'll probably be easier to clean, though for the life of me I cant figure out why you'd want to clean the curing out of a smoker. You might have some flaking where you weld, but it wont go far. Use the tank. You'll be fine.
__________________
There are no problems. There are only solutions. It's your duty to determine the right one.

Hobart Handler 210
Airco 225 Amp MSM Stinger
Reply With Quote
  #19  
Old 07-23-2012, 08:50 PM
Bistineau's Avatar
Bistineau Bistineau is offline
WeldingWeb Craftsman
 
Join Date: Jul 2011
Location: Bossier Parish La.
Posts: 1,069
Re: Bbq/smoker question

Quote:
Originally Posted by ThorsHammer View Post
Why not use it if it's ceramic? your house hold oven is ceramic lined. It's cooking at higher temps just fine. so you would have nothing to worry about with your offset. the ceramic is going to be harder, and last longer than anything else that could be put in it. not to mention it'll probably be easier to clean, though for the life of me I cant figure out why you'd want to clean the curing out of a smoker. You might have some flaking where you weld, but it wont go far. Use the tank. You'll be fine.
I'm in agreement with Thorshammer, if the heat of a torch won't make it come loose then the heat of cooking won't either as it's much lower. Just don't build a trailer to carry it on with a 120V MIG welder.
Reply With Quote
  #20  
Old 07-23-2012, 11:30 PM
Jwgrillin Jwgrillin is offline
Solderer
 
Join Date: Jul 2012
Posts: 7
Re: Bbq/smoker question

Quote:
Originally Posted by Bistineau View Post
I'm in agreement with Thorshammer, if the heat of a torch won't make it come loose then the heat of cooking won't either as it's much lower. Just don't build a trailer to carry it on with a 120V MIG welder.
I smacked the tacks off the legs tonight with a sledge, and put the tank out back for now. I gonna try a double barrel smoker/que. My boss gave me 3 drums today so Ill start with that.. Meanwhile my uncle is on the lookout for me to fine a 150-250 gallon propane tank. That way I can build my ultimate smoker/que
__________________
Miller Millermatic 252
Hypertherm plasma
Reply With Quote
  #21  
Old 07-24-2012, 01:09 PM
ThorsHammer's Avatar
ThorsHammer ThorsHammer is offline
WeldingWeb Artisan
 
Join Date: Jul 2011
Location: Western Washington
Posts: 2,099
Re: Bbq/smoker question

do a Search for Fafnir and you'll find my DBS build.
__________________
There are no problems. There are only solutions. It's your duty to determine the right one.

Hobart Handler 210
Airco 225 Amp MSM Stinger
Reply With Quote
  #22  
Old 12-24-2012, 07:09 AM
jaxerozen jaxerozen is offline
Solderer
 
Join Date: Dec 2012
Posts: 1
Re: Bbq/smoker question

It is really important to paint inside of the smoker to maintain it for long. I am using my bbq griller cum smoker from about ten years. It is in very good condition. I then realized it is because of the bbq smoker paint which we have used to it. You can use rust-o-leum 1000 degree, or 1300 degree which can resist temperature and also non-toxic.
__________________
bbq smokers
bbq grills smokers
Reply With Quote
  #23  
Old 12-24-2012, 08:23 AM
MarkBall2's Avatar
MarkBall2 MarkBall2 is offline
WeldingWeb Artisan
 
Join Date: Apr 2008
Location: Yuma AZ
Posts: 2,290
Re: Bbq/smoker question

Why paint the inside. A smoker will get covered with soot & if you had applied any veggie oil/lard to season it, it won't rust through.

I would only season it, as that's all it really needs. Many of the propane tank builds have been in service for years without any rusting.

Here are some ideas for the barrel smokers: (The 3rd one is mine)
Attached Images
     
__________________
Mark
I haven't always been a nurse........

Craftsman 12"x36" Lathe
Enco G-30B Mill
Hobart Handler 175
Century 230 Amp A/C stick welder
Chicago Electric 165A DC TIG
Oxy/Acetylene set
PapaLion's Gate Build
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 04:23 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.