Powermax 65 csa CPC voltage divider option

Hi All,
I have a PM65 and at this moment I would like to read the voltage from the CPC option. As I read at the manual, it says that it is possible to have 18 Volts maximum at the CPC.
I dont understand why, because if I set the switch to read 1:50 from the raw arc, thats means 50X18 Volts=900 Volts at the torch.

Is my math wrong?
It is important to know about it, because I want to use a device that reads maximum 10 Volts.
Thanks in advance for your help
__________________
Mauricio
Reply With Quote
  #2  
Old 07-30-2012, 12:17 AM
ccawgc ccawgc is offline
WeldingWeb Artisan
 
Join Date: Mar 2010
Location: Ceres, California
Posts: 2,003
Re: Powermax 65 csa CPC voltage divider option

Call Hypertherm tech support and ask. make sure you are reading the manual correctly so nothing gets fried.
Reply With Quote
  #3  
Old 07-31-2012, 07:54 AM
pandinus pandinus is offline
WeldingWeb Journeyman
 
Join Date: Mar 2010
Posts: 75
Re: Powermax 65 csa CPC voltage divider option

I "believe" that the 18V would be at 20:1 (least reduction) .... so ... 360V/20 = 18V

then at 50:1 360V/50V = 7.2V ... so at 50:1 the max out of the divider should be 7.2V

I'm sure Jim will confirm or correct this...
__________________
Never argue with an idiot. They drag you down to their level, then beat you with years of experience.
Reply With Quote
  #4  
Old 07-31-2012, 06:50 PM
mauricio_daniel_62's Avatar
mauricio_daniel_62 mauricio_daniel_62 is offline
WeldingWeb Tradesman
 
Join Date: Feb 2010
Location: BA, AR
Posts: 256
Re: Powermax 65 csa CPC voltage divider option

Thanks for your help. I think that you're right. I will test using 1:50, and measuring the voltage at the CPC.
Best Regards
__________________
Mauricio
Reply With Quote
  #5  
Old 08-01-2012, 09:36 AM
jimcolt jimcolt is offline
WeldingWeb Craftsman
 
Join Date: Oct 2007
Location: New Hampshire
Posts: 1,662
Re: Powermax 65 csa CPC voltage divider option

Pandinus is correct. The CPC (circular plastic connector) voltage divider output as used on the Hypertherm Powermax65, 85 and 105 has 5 settable outputs which are: 20:1, 21.1:1, 30:1, 40:1 and 50:1. At the lowest numeric setting (20:1) under open circuit voltage conditions in the power supply...there could be as much as 18 volts DC present on pins 5 (negative) and 6 (positive) of the CPC connector.

Jim Colt


Quote:
Originally Posted by mauricio_daniel_62 View Post
Thanks for your help. I think that you're right. I will test using 1:50, and measuring the voltage at the CPC.
Best Regards
Reply With Quote
  #6  
Old 08-01-2012, 11:11 AM
mauricio_daniel_62's Avatar
mauricio_daniel_62 mauricio_daniel_62 is offline
WeldingWeb Tradesman
 
Join Date: Feb 2010
Location: BA, AR
Posts: 256
Re: Powermax 65 csa CPC voltage divider option

Hello Jim,
Thanks for your reply. This weekend I will set the output at the 50:1 option.
After this using a DC multimeter I will test the output voltage at the CPC at open circuit and also making some cuts with differents torch heights.
I´ll keep you posted.
Best Regards
__________________
Mauricio
Reply With Quote
  #7  
Old 08-01-2012, 11:22 AM
jimcolt jimcolt is offline
WeldingWeb Craftsman
 
Join Date: Oct 2007
Location: New Hampshire
Posts: 1,662
Re: Powermax 65 csa CPC voltage divider option

In the Powermax units you will not be able to read open circuit voltage unless the torch has consumables that are stuck open. Under normal conditions the electrode (negative ) and nozzle (positive) are shorted when the torch is first triggered (this is when the open circuit could occur)...then when air pressure rises in the torch the electrode pulls away from the nozzle....the system establishes a pilot arc (which will produce a lower voltage than an open circuit voltage)....then if close to the plate (attached to the work ground) will establish a transfered arc.

The best way to determine if the voltage divider is working properly is to measure the raw DC voltage and compare that to the divided output voltage real time while cutting.

Jim Colt


Quote:
Originally Posted by mauricio_daniel_62 View Post
Hello Jim,
Thanks for your reply. This weekend I will set the output at the 50:1 option.
After this using a DC multimeter I will test the output voltage at the CPC at open circuit and also making some cuts with differents torch heights.
I´ll keep you posted.
Best Regards
Reply With Quote
  #8  
Old 08-01-2012, 05:47 PM
mauricio_daniel_62's Avatar
mauricio_daniel_62 mauricio_daniel_62 is offline
WeldingWeb Tradesman
 
Join Date: Feb 2010
Location: BA, AR
Posts: 256
Re: Powermax 65 csa CPC voltage divider option

Hi Jim,
Thanks again for your comments, helps me a lot.
Best Regards
__________________
Mauricio
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump


All times are GMT -4. The time now is 08:17 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.