#1  
Old 08-09-2012, 07:54 AM
Jeff F. Jeff F. is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Posts: 13
6G GMAW Cert Test

I have to take my 6G today and I'm super nervous. I'll be taking the test with .035 and 75/25. Is there a ball park v/a setting that you might suggest for a good root pass. Any tips or tricks sincerely appreciated. I've scoured the internet and most advice is on stick! Thanks!
Reply With Quote
  #2  
Old 08-09-2012, 08:25 AM
hobohilton's Avatar
hobohilton hobohilton is offline
WeldingWeb Foreman
 
Join Date: Dec 2010
Location: Pacific Northwest
Posts: 817
Re: 6G GMAW Cert Test

What code will you be certifying to?

Thanks,

Hobo
__________________
Lincoln SA200's... at least 15 - 20. They come and go. Growing partial to the "Short Hoods" in my old age. Last count on Short Hoods was 13 in possession.
Reply With Quote
  #3  
Old 08-09-2012, 08:29 AM
ironrail ironrail is offline
WeldingWeb Journeyman
 
Join Date: Jan 2012
Posts: 94
Re: 6G GMAW Cert Test

Have you been practicing? If so,don't try anything new on your test.
Reply With Quote
  #4  
Old 08-09-2012, 08:29 AM
Jeff F. Jeff F. is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Posts: 13
Re: 6G GMAW Cert Test

ASME. And it will all be uphill.
Reply With Quote
  #5  
Old 08-09-2012, 07:12 PM
Welding_Swede's Avatar
Welding_Swede Welding_Swede is offline
WeldingWeb Tradesman
 
Join Date: Jan 2011
Location: South East Michigan
Posts: 293
Re: 6G GMAW Cert Test

If its 6G then how can it be uphill? Well, some of it yes. But some of down, flat, etc.

Short circuit GMAW for ASME pressure pipe? Are you sure?

Eric
__________________
AWS D1.1 Certified SMAW 3G Unlimited, Open Root
FCAW 3G Unlimited, w/Backer
AWS D1.2 Certified GMAW Aluminum 3G 1/2"
GTAW Aluminum 3G 1/2"
Reply With Quote
  #6  
Old 08-17-2012, 03:31 PM
Jeff F. Jeff F. is offline
WeldingWeb Apprentice
 
Join Date: Jan 2012
Posts: 13
Re: 6G GMAW Cert Test

Quote:
Originally Posted by Welding_Swede View Post
If its 6G then how can it be uphill? Well, some of it yes. But some of down, flat, etc.

Short circuit GMAW for ASME pressure pipe? Are you sure?

Eric
Should have said some of it was uphill. It was a fixed 45 degree around the pipe. And yes, we test with mig. I wasn't quite ready for it. First three passes weren't bad but my cover wasn't so pretty. Didn't even bother getting it cut up. Need some more practice.Never did anything like that before in my 20 years of welding. Gotta get a better technique for puddle control on my bad side of the bottom to midway mark. It was a learning experience though, so not a total loss.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:27 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.