Any help on vertical mig welding on a miller 400 440 volt with 0.045 solid core wire.
Reply With Quote
  #2  
Old 04-02-2009, 01:37 AM
DesertRider33's Avatar
DesertRider33 DesertRider33 is offline
Master Welder
 
Join Date: Oct 2006
Location: Ca, USA
Posts: 5,242
Re: Vertical Mig

Set heat a little lower than you would for flat position. Point torch slightly up. Start at bottom of joint and work up. As you move up, move the torch slightly side to side within the puddle. Hold momentarily at the sides and zip accross the middle. Holding the sides helps the toes fill and zipping accross the middle keeps the middle from humping up. Move up in small increments.
__________________
MM350P/Python/Q300
MM175/Q300
DialarcHF

HTP MIG200
PowCon300SM

Hypertherm380
ThermalArc185
Purox oa
F350CrewCab4x4
LoadNGo utilitybed
Bobcat250
XMT304/Optima/Spoolmatic
Suitcase12RC/Q300
Suitcase8RC/Q400
Passport/Q300

Smith op
Reply With Quote
  #3  
Old 04-14-2009, 03:54 AM
chrispc66 chrispc66 is offline
WeldingWeb Journeyman
 
Join Date: Jul 2008
Posts: 109
Re: Vertical Mig

Pulsed GMAW is far superior for VU GMAW applications. If you are stuck with rectifying power sources, perhaps VD may be more suited.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 07:14 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.