Miller 225D Plus
As I mentioned in my intro, I aquired a Bobcat 225D Plus from my office. It wasn't running and ended up being a stuck injector pump which in turn made the fuel rack itself stick too. Got it running last Tuesday and Sunday I plan to try and weld with it. Below are a couple questions I have about it.
1. How can I remove the fuel tank to try and clean it? Can it come out the bottom or a side so that I don't have to remove all the electrical items? If no, then I'll just run some clean diesel through it and keep a couple spare filters on standby. 2. I'm being told it wouldn't keep a battery. In the manual it says to check the voltage regulator. How can I check this? 3. I'm being told that when it was last being used here (upwards of 2-3 years ago) it would tack good with stick, but it wouldn't weld consistantly. Any thoughts on this? 4. I want to get a wire feeder for it. Local store quoted me a Suitcase X-Treme 12VS, but that is way out my price range, considering I got the machine for free, so is there an older wire feeder model that I can use that I can find a used one? |
|
#2
|
||||
|
||||
|
Re: Miller 225D Plus
On the wire feeder, look around for a used Lincoln LN25 or Hobart Hefty or Miller Suitcase VS. My first Suitcase 8VS I bought used in great condition for $500. Found it on Craigs List.
__________________
MM350P/Python/Reach/Q400 MM175/Q300 DialarcHF HTP MIG200 PowCon 300SM HyperthermPM380 ThermalArc185 Victor o/a -F350 CrewCab4x4 -LoadNGo utilitybed -Bobcat250NT -XMT304/Optima/XR/Spoolmatic -Suitcase8RC/Q300 -Passport/Q300 -JacksonEQC |
|
#3
|
|||
|
|||
|
Re: Miller 225D Plus
I have an old Miller Super S-32P that is a VS type feeder. I picked it up used for about what DR got his for, from a place that refurb'd it.
__________________
. No government ever voluntarily reduces itself in size. Government programs, once launched, never disappear. Actually, a government bureau is the nearest thing to eternal life we'll ever see on this earth! Ronald Reagan |
|
#4
|
|||
|
|||
|
Re: Miller 225D Plus
We have an SP model, I think its an SP-32P as well, in our shop and I'm wondering if I can use one of those on this machine. I know I can find those at a decent price.
|
|
#5
|
||||
|
||||
|
Re: Miller 225D Plus
You can use any volt-sensing non-remote feeder on your Bobcat. Don't buy any feeders that have a 14-pin remote control cable and you'll be fine.
__________________
MM350P/Python/Reach/Q400 MM175/Q300 DialarcHF HTP MIG200 PowCon 300SM HyperthermPM380 ThermalArc185 Victor o/a -F350 CrewCab4x4 -LoadNGo utilitybed -Bobcat250NT -XMT304/Optima/XR/Spoolmatic -Suitcase8RC/Q300 -Passport/Q300 -JacksonEQC |
|
#6
|
||||
|
||||
|
Re: Miller 225D Plus
Don't waste your time with the wire feeder for your 225 bobcat. I have an extreme 12vs and my old 225 would not run the feeder. The older 225 do not make enough CV power to run a 12vs, unless you run .023 wire.
__________________
Xtreme Fabrication Lincoln 300 Commander Miller -Syncrowave 200 -XMT350MPA -Xtreme 12vs -Millermatic 210 w/3035 -Dialarc 250 -52 Spot Victor torches Hypertherm 1250 Rockwell 9 Bandsaw GEKA 50A 60 ton and Bantom 10 ton Ironwokers |
|
#7
|
||||
|
||||
|
Re: Miller 225D Plus
My buddy has a late 90's Bobcat 225NT and runs fluxcore .045 with it in a 12VS no problems.
__________________
MM350P/Python/Reach/Q400 MM175/Q300 DialarcHF HTP MIG200 PowCon 300SM HyperthermPM380 ThermalArc185 Victor o/a -F350 CrewCab4x4 -LoadNGo utilitybed -Bobcat250NT -XMT304/Optima/XR/Spoolmatic -Suitcase8RC/Q300 -Passport/Q300 -JacksonEQC |
|
#8
|
|||
|
|||
|
Re: Miller 225D Plus
Struck an arc with the Bobcat yesterday. Burnt one rod of LH just welding on some angle. Would weld a little and stop and the engine would idle down. Arc again and it would speed up. Seems to weld pretty good for not being used in almost 2 or 3 years.
Going to hook the leads to my dad's SP-32P and see how the bobcat handles it. If it does good, then I'll just find a used one somewhere instead of getting the X-treme that is way out of my price range. |
![]() |