A question on tig welding aluminum.....using 3/32 green tungston with 3/32 4043 filler ,,,,welding .125 ga al......i'm am alright after i get the material tacked togather.i am just practicing making cubes. I seem to have problems getting the material tacked togather. I try to let the aluminum get shinny,ready to accept the filler and sometime everything goes well,and sometimes the ouside corner mostly acts like it has became containmaneted or something....looks like ****...the outside corners are the worst about this..i have all the setting in auto using pure argon flow set at about 15 i tried lowering amps,raising amps,,,,,,,,like i said sometimes it works fine,sometimes not..and when you try to weld over these ****ty tacks,most of the time is looks no good...if i can get this part straighten out,then i will feel 100% better,,,,,,,,,,any help on putting tacks on outside corners on aluminum now once i get rolling it looks sweet....i have a lincoln 275 preision tig if this helps,built in pulse,with the advance control panel.........please help on outside corners tacking????????????????????aluminum thanks
Reply With Quote
  #2  
Old 06-08-2010, 01:37 AM
Rojodiablo's Avatar
Rojodiablo Rojodiablo is offline
Master Welder
 
Join Date: Feb 2006
Location: Back in HB, close to my boys!!
Posts: 4,457
Re: Tig welding help????????????

That is a function of foot pedal ramping, and also, more importantly, where and how you are dropping your filler in. I'll try to explain: If the filler rod is kept really close to the puddle, it will heat up, and turn into the blob before you can make a clean dab with it. Now, let's say you get it about 1/2" from the arc. Form a puddle, and then move the filler in smooth and quickly to the puddle. Make a dab, and back the pedal off about 1/2 or so, so the puddle will cool a bit. As you do this, only pull that filler rod back about 1/4". As you ramp up the amps, and move the torch forward, make another dab. Then, back out of it, and let the tack cool.
Try to get a good fit up on your parts; it's awful hard to get a clean puddle across a gap of even 1/16" with thin aluminum.
__________________
I think she is Bi-polar. She is a bear sometimes. Does this make her a BiPolar bear????
Reply With Quote
  #3  
Old 06-08-2010, 02:32 AM
thermalfusioneng. thermalfusioneng. is offline
WeldingWeb Journeyman
 
Join Date: Aug 2009
Location: Ca,
Posts: 84
Re: Tig welding help????????????

Brother you shoud try a little mek to get the residues off the material. Then hit it with a wire brush. I would get rid of the green puretung unless you are getting into some boeing spec work. Try some thoriated tungsten 2% you pretty much can do it all with that stuff . set your gas at 20 #5 cup. You should be welding like a pro in about a minute.
Reply With Quote
  #4  
Old 06-08-2010, 04:41 AM
wareagle wareagle is offline
WeldingWeb Journeyman
 
Join Date: Jan 2009
Location: lawrenceburg,ky
Posts: 69
Re: Tig welding help????????????

okey thank you for the advise...i will try some red tungstons out,and a little more gas!!!!! no doubt aluminum sucks with poor fit ups. thank you for the advise and keep them comming!!!!! thank you all 4 any help
Reply With Quote
  #5  
Old 06-08-2010, 05:21 AM
wareagle wareagle is offline
WeldingWeb Journeyman
 
Join Date: Jan 2009
Location: lawrenceburg,ky
Posts: 69
Re: Tig welding help????????????

just another question to throw at you all,,,,,,,,,,,,why would welding w/a red tungston benifit me more than a green tungston???? i was just wondering for my benifit?well i'm going out to the garage right this second to tackel this,,,,,,,,,,,,,,,,once again thanks for any help you guy share!!!
Reply With Quote
  #6  
Old 06-08-2010, 07:05 AM
sn0border88 sn0border88 is offline
WeldingWeb Artisan
 
Join Date: Aug 2007
Posts: 1,765
Re: Tig welding help????????????

Short answer, red TUNGSTEN has a higher melting point and will handle the amps better. Meaning it will hold a point and give you more control over the arc than pure.

Try decreasing your stickout to as short as you can manage. I found this to be one of the most helpful things on AL. I would also go to a larger cup than a #5, thats pretty small. If you have a #8 it will work better.
__________________
Have we all gone mad?
Reply With Quote
  #7  
Old 06-08-2010, 11:32 AM
wareagle wareagle is offline
WeldingWeb Journeyman
 
Join Date: Jan 2009
Location: lawrenceburg,ky
Posts: 69
Re: Tig welding help????????????

thankyou for all the info,,,,,i done alot better now,,,,a good fit up was my main problem i guess.. the red tungston worked out pretty good too. when you are doing real important aluminum welding,,,,,,like x-ray type would you then use a green/pure tungston????is it still okey to use red???? my aluminum is in pretty good condition...do you guys still clean it with anything,sand/grind,or wire brush before welding???????and if so whats some tips to use??? thanks
Reply With Quote
  #8  
Old 06-08-2010, 07:01 PM
weregeek weregeek is online now
WeldingWeb Journeyman
 
Join Date: Nov 2008
Location: Grinnell, IA
Posts: 53
Re: Tig welding help????????????

I generally remove the oxide layer in the joint area with a stainless brush used only for aluminum, and clean the weld area and filler with acetone prior to striking an arc. This goes a long way to keeping those little black specs out of the weld pool.

If your problems don't disappear after applying the tips above, you may need to take a look at shielding gas coverage.
Reply With Quote
  #9  
Old 06-09-2010, 01:20 AM
Rojodiablo's Avatar
Rojodiablo Rojodiablo is offline
Master Welder
 
Join Date: Feb 2006
Location: Back in HB, close to my boys!!
Posts: 4,457
Re: Tig welding help????????????

Quote:
Originally Posted by wareagle View Post
thankyou for all the info,,,,,i done alot better now,,,,a good fit up was my main problem i guess.. the red tungston worked out pretty good too. when you are doing real important aluminum welding,,,,,,like x-ray type would you then use a green/pure tungston????is it still okey to use red???? my aluminum is in pretty good condition...do you guys still clean it with anything,sand/grind,or wire brush before welding???????and if so whats some tips to use??? thanks
Fit up is everything, with the exception of cleaning!!! To clean it up, use a SS wire brush. Scrub off the oxide, it will be clean and shiny. AMAZING difference.

As for the difference between tungstens, the green was the staple, and is still the one to use on the old machines. The advent of more advanced wave shapes, sharper arcs, different HF start systems have given the opportunity to use different tungstens for aluminum. Red, orange, gold tungstens all work pretty well. Red will split and crack with high amps. Easy fix, re-grind and go. All the blended tungstens will hold up to high amps a bit better, and can give a sharper arc. The blended tungstens will hold up to mistakes a lot better than pure tungsten. A dip with a liquid ball of green tungsten guarantees a big mess in the material. With red, you usually only coat the tungsten with aluminum, and maybe a little tungsten contamination. (You need to clean that out of the aluminum and start over if you dunk it hard....)
__________________
I think she is Bi-polar. She is a bear sometimes. Does this make her a BiPolar bear????
Reply With Quote
  #10  
Old 06-11-2010, 11:32 AM
thermalfusioneng. thermalfusioneng. is offline
WeldingWeb Journeyman
 
Join Date: Aug 2009
Location: Ca,
Posts: 84
Re: Tig welding help????????????

Good answers to this guys questions, but now I have a question. Do any of you welders ever ball up the tungsten over a copper block before you weld? I dont know thats how we used to do it before inverter type welders. When you ball up the tungsten to the same dia as your tung electrode, there is no wandering arc.
The gas, it just simply spins around the ball on your tungsten.Thus a wider arc gas cone and a more stable arc.
Reply With Quote
  #11  
Old 06-11-2010, 11:51 AM
zapster's Avatar
zapster zapster is offline
Moderator
 
Join Date: Jan 2006
Location: In A Nice Comfy Chair
Posts: 13,961
Re: Tig welding help????????????

Quote:
Originally Posted by thermalfusioneng. View Post
Good answers to this guys questions, but now I have a question. Do any of you welders ever ball up the tungsten over a copper block before you weld?

Nope..
I just grind it to a point then weld away until the "Ball" gets about the size on the tungston (3/32") then sharpen all over again..
Or switch out to ones that already have been sharpened..

...zap!
__________________


I am not completely insane..
Some parts are missing

I have figured out that keeping everyone happy is nearly impossible but pissing people off is easy and fun.
Reply With Quote
  #12  
Old 06-11-2010, 11:57 AM
thermalfusioneng. thermalfusioneng. is offline
WeldingWeb Journeyman
 
Join Date: Aug 2009
Location: Ca,
Posts: 84
Re: Tig welding help????????????

You know the last time I welded aluminum with a pointed tungsten ( yesterday) it was for welding 2" thick aluminum. The procedure was straight helium set your gas @45 and machine on dc straight just like when your welding steel or stainless. Thats if you have a small machine you know like a lincoln 175. your welds will be smaller and the haz (heat affected zone) will not change the molecular property of your aluminum.Plus you can travel the puddle at higher rates thus faster cooling. Rule of thumb .020 aluminum thru .187 ac welding w/argon .187 thru .375 ac w/ helium argon. .375 thru unlimited dc weldingw straight helium. Adjust your tungsten dia as the material gets thicker but with dc welding a 1/8 tung will do. Have fun exploring your newly taught parameters. Go get em, LOL
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 02:05 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.