Chineese Stainless welding Quest.
I do not post here much, but I lurk around here a lot. I just got a Miller 180SD syncrowave machine. I am practicing as much as I can. I have a job to weld some stainless for the club/bar I bounce at. They asked me to weld some stainless rod to a stainless Ice bucket. These rods will be bent in a way that they will hold small bottles (3 attached to each bucket 120 degrees apart). They supplied me with the stainless bucket. On the bottom of the bucket is made in China and it says "stainless 10/18". I already made a jig to bend the .250 308 Rod. What filler should I use to weld the rod to the bucket. I am thinking 308 filler. Hard to explain what I am doing but I will post a pic when I bend the rod tomorrow.
Thanks
T.J.
|