how are my welds looking?
Hi Gang,
My first post here and I wanted to share some of my latest work. I am using a synchrowave 180 and the material is .083 chrome-moly tubing. The machine is set to DC, 85amps, argon set to 15cfh, tungsten is 1/16 with a gas lens and I am using ER80SD2 as filler. I don't have much experience with TIG, about 15-20hrs. actual welding time. But I was hoping to get some feedback about what I could be doing better or what suggestions I could learn from. Thanks in advance.
-Brian
"newbie tig welder"
|