1" Steel Plate

Hello,

I'm a small excavating contractor in North Central N.J. I have one machine with a few attachments. I would like to store the attachments on a 1" x 8' W x 15' L plate so I can move them all in one pick. I've received prices around 30/s.f. which seems quite expensive. Can anyone tell me if there is a used market for this?

Thank You in advance

Frank
Reply With Quote
  #2  
Old 04-02-2012, 02:05 PM
morgaj1's Avatar
morgaj1 morgaj1 is offline
WeldingWeb Tradesman
 
Join Date: May 2011
Location: Alabama
Posts: 377
Re: 1" Steel Plate

That works out to $0.75/lb. Around here in AL, the going rate for plate steel is about $0.65. However, steel prices vary all around the country.
__________________
Lincoln Powermig 255
Hypertherm Powermax 45
Thermal Arc 161S
Oxweld 24R OA Torch
Still Looking for an Old Round Top Idealarc 250
Reply With Quote
  #3  
Old 04-02-2012, 02:59 PM
sn0border88 sn0border88 is offline
WeldingWeb Artisan
 
Join Date: Aug 2007
Posts: 1,765
Re: 1" Steel Plate

The only used market you are going to find would be a scrap yard, go to one that lets you look around and see if you can find plate that will suite your needs.
__________________
Have we all gone mad?
Reply With Quote
  #4  
Old 04-02-2012, 03:24 PM
forhire's Avatar
forhire forhire is online now
WeldingWeb Artisan
 
Join Date: Mar 2010
Location: Morton, Washington
Posts: 2,466
Re: 1" Steel Plate

Steel is generally sold by the pound (actually hundred weight), in your example that's $75 per hundred or 0.75/lb. I get real nervous when I'm quoted by the square foot.

My price on some wide beam last week was around $57 per 100.

For plate I've been using Chapel Steel out of Portland, OR. They have a location in Philadelphia, PA... not sure if that's too far for you. Might give them a call. Trucking is really driving the material costs. Find a yard that brings it in by rail and your cost will generally be lower. http://www.chapelsteel.com/locations.html

I hope your planning on supporting this plate on some beams... even 1" plate is like spaghetti.
Reply With Quote
  #5  
Old 04-02-2012, 03:50 PM
ironmangq ironmangq is offline
WeldingWeb Foreman
 
Join Date: Feb 2010
Posts: 662
Re: 1" Steel Plate

I would look into building a frame to carry the implements rather than a piece of plate, It will be stiffer and probably easier to move around
Reply With Quote
  #6  
Old 04-02-2012, 04:29 PM
Fat Bastard's Avatar
Fat Bastard Fat Bastard is offline
Master Welder
 
Join Date: Jul 2008
Location: Anchorage Alaska
Posts: 3,644
Re: 1" Steel Plate

$75.00 CWT is what I'm paying in Alaska. So $75.00 CWT in the 48 is high way high.
__________________
Brucy is an admitted unemployment cheat. AND he is PROUD of it. Kentucky should be proud. Shame on you Bruce.
Prophet Mohammed, womanizer, child molester and ruthless killer?
Reply With Quote
  #7  
Old 04-02-2012, 05:12 PM
Mondo's Avatar
Mondo Mondo is offline
WeldingWeb Craftsman
 
Join Date: Feb 2008
Location: NH no mo - MA now.
Posts: 1,372
Re: 1" Steel Plate

The price you were quoted is probably about right, this is a big chunk of steel. 4'x8' is probably less per pound or sq ft.

Have you really thought this through and considered the weight? You want to store all your "small" machine implements on one plate for easy moving, right?

1" plate is 40.8 lbs/sqft. (http://www.engineeringtoolbox.com/st...ht-d_1561.html) You said 8' x 15' That's 120 sqft
120 x 40.80 = 4,896 lbs. To handle this flat will be like handling a sheet of paper from a note pad unless it has substantial support secured beneath it. Add the weight of the support framing, add the weight of the stuff you intend to store/move on it and you are going to have a rather heavy load. What kind of machinery do you have to handle this load? When you say you want to move it "in one pick" I presume you mean by crane. A big crane.

Oh yes, I need to mention also that you need to provide some means of securing each implement to the plate lest it slide like an omelet off a greasy spatula! I'll watch from a vantage point in the next county.

I am sure this can be done but unless you always work large sites that have one or more big cranes I don't see this as practical.

- Mondo
__________________
Member, AWS
Lincoln ProMIG 140
Lincoln AC Tombstone
Craftsman Lathe 12 x 24 c1935
Craftsman Commercial Lathe 12 x 36 c1970
- - -
Ask for a wrench and someone will offer you a grinder.
I'll just keep on keepin' on.
Reply With Quote
  #8  
Old 04-02-2012, 05:17 PM
Mondo's Avatar
Mondo Mondo is offline
WeldingWeb Craftsman
 
Join Date: Feb 2008
Location: NH no mo - MA now.
Posts: 1,372
Re: 1" Steel Plate

For what it is worth have you considered keeping the implements secured to a flat or gooseneck trailer and having the crane pick the trailer?

- Mondo
__________________
Member, AWS
Lincoln ProMIG 140
Lincoln AC Tombstone
Craftsman Lathe 12 x 24 c1935
Craftsman Commercial Lathe 12 x 36 c1970
- - -
Ask for a wrench and someone will offer you a grinder.
I'll just keep on keepin' on.
Reply With Quote
  #9  
Old 04-02-2012, 05:36 PM
Pavinsteelman Pavinsteelman is offline
WeldingWeb Tradesman
 
Join Date: Feb 2011
Location: South Plainfield NJ
Posts: 335
Re: 1" Steel Plate

Hi 4900 lbs mill price is .52 lb plus frt . try Joseph Fazzio in so jersey for used plate.People paid almost 1.00 lb at Ace Manzo auction in NJ for road plates .
Reply With Quote
  #10  
Old 04-02-2012, 09:28 PM
pslwelder pslwelder is offline
WeldingWeb Apprentice
 
Join Date: Mar 2012
Posts: 45
Re: 1" Steel Plate

I'll second Fazio's. Price's are fair and huge stock. I believe they have a store at the RT.33-34 circle in wall.
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 10:20 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.