#1  
Old 08-11-2012, 09:30 PM
ChisolmCreekServices ChisolmCreekServices is offline
Solderer
 
Join Date: Aug 2012
Location: Oklahoma
Posts: 2
Miller Bluestar 2E

My machine will start and run great
for about 5 min. then it dies. It does the
Same thing on high idle and auto.
Have fuel, fire, and spark. Is there some
Electrical part that I could check out?
Reply With Quote
  #2  
Old 08-12-2012, 08:47 AM
mla2ofus mla2ofus is offline
WeldingWeb Artisan
 
Join Date: Apr 2006
Location: Soda springs,Id
Posts: 2,269
Re: Miller Bluestar 2E

Are you certain it's still getting fuel and spark at the moment it dies? Have you done a compression test immediately after it dies?

Mike
__________________
Ol' Stonebreaker
"Experience is the name everyone gives to their mistakes"

Miller 175 mig
Miller thunderbolt ac/dc stick
Victor O/A setup
Makita chop saw
Reply With Quote
  #3  
Old 08-12-2012, 09:12 AM
anickode anickode is offline
WeldingWeb Foreman
 
Join Date: Mar 2012
Posts: 557
Re: Miller Bluestar 2E

Will it restart after it dies with minimal cool down time?

If so, I'd be looking at a fuel clog, sunken carb floats, or mechanical vibration causing a short in the ignition system or p-lead
__________________
You didn't build that.

'85 Miller AEAD-200LE

Last edited by anickode; 08-12-2012 at 09:14 AM.
Reply With Quote
  #4  
Old 08-12-2012, 09:37 AM
Tool Maker Tool Maker is offline
WeldingWeb Foreman
 
Join Date: Jun 2011
Location: Oregon
Posts: 500
Re: Miller Bluestar 2E

It definatly sounds like fuel Problem anyway. mac
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is Off
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 01:35 AM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.