used flow meter?
looking for a decent flow meter for argon. i saw the cga 580 is cheap, but are there that many differences in brands? If anyone has a one laying around and dosnt want a ton of $ for it let me know. also, still looking for 14 pin foot pedal. thanks, Joe
|
|
#2
|
|||
|
|||
|
Re: used flow meter?
" CGA-580" is the inlet fitting size you need, not a model number.
|
|
#3
|
||||
|
||||
|
Re: used flow meter?
I would sell one for $50 including shipping.
__________________
Dynasty 200DX Passport plus w/ spoolmate 100 victor 315c oxy/(act and prop) Miller digital elite milwaukee power tools |
|
#4
|
|||
|
|||
|
Re: used flow meter?
|
|
#5
|
|||
|
|||
|
Re: used flow meter?
thanks MX, and Turk!
|
|
#6
|
|||
|
|||
|
Re: used flow meter?
__________________
First-born son: KIA Iraq 1/26/05 Syncrowave 250 w/ Coolmate 3 Dialarc 250 SP-175 + TA 161 STL Lincwelder AC180C (1952) Victor & Smith O/A torches Miller spot welder Clausing 5904 lathe Wells-Index 745 mill |
|
#7
|
|||
|
|||
|
Re: used flow meter?
Thanks guys. I got a used víctor for 29.99 on ebay
|
![]() |