What am I doing wrong? Please help

I am welding some .125 cold steel and all my welds are looking like popcorn. It seems nice untill I hammer the slag off and then it looks nasty like it caved in or something. My straight welds come out just fine, only having this problem on a 90 degree weld. Currently I'm using 6013 but 7018 and 6011 are doing the same thing. I am running about 80 - 90 amps AC.

Thanks
Reply With Quote
  #2  
Old 08-08-2004, 09:16 PM
HWooldridge HWooldridge is offline
WeldingWeb Journeyman
 
Join Date: Mar 2004
Location: Central Texas
Posts: 136
Turn up the juice a bit - maybe 110 to 120. Fillet welds take a little more amperage.
__________________
Get it hot and hit it hard...
Reply With Quote
  #3  
Old 08-08-2004, 10:13 PM
Benny Benny is offline
WeldingWeb Apprentice
 
Join Date: Mar 2004
Posts: 18
I try that.
Thanks
Reply With Quote
  #4  
Old 08-09-2004, 10:43 PM
Benny Benny is offline
WeldingWeb Apprentice
 
Join Date: Mar 2004
Posts: 18
Good call
Cranked it up and now I'm getting much better welds

Thanks again
Reply With Quote
Reply

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -4. The time now is 09:02 PM.


Powered by vBulletin® Version 3.8.7
Copyright ©2000 - 2013, vBulletin Solutions, Inc.
Copyright ©2000 - 2013, Penton Media, Inc. All rights reserved.