Which Grade of mild steel??

just wondering which grade of mild carbon steel is ideal for building utility (quad) trailers??

any help is appreciated
Reply With Quote
  #2  
Old 10-13-2004, 07:36 PM
boilerman79 boilerman79 is offline
WeldingWeb Journeyman
 
Join Date: Mar 2004
Location: virginia
Posts: 86
A36 is the most common grade.