Motorcycle 11 inch cutout
I cut this today just messing around with my CNC table. I only had a piece of metal 12" wide so I resized the file from 22" to 11". In doing so, some of the inside details fell out when cutting as I knew they would. Still not a bad cut with no problems with lost steps.
Plasma is Longevity Force Cut LP80D at 35 amps with 75 PSI air. Metal is aluminum 3/32". I did no cleanup on this piece since it was just a test and will go in the recycle bin.
Dan